Journal of Ceramic Science and Technology

The Journal of Ceramic Science and Technology publishes original scientific articles on all topics of ceramic science and technology from all ceramic branches. The focus is on the scientific exploration of  the relationships between processing, microstructure and properties of sintered ceramic materials as well as on new processing routes for innovative ceramic materials. The papers may have either theoretical or experimental background. A high quality of publications will be guaranteed by a thorough double blind peer review process.

The Journal is published by Göller Verlag GmbH on behalf of the Deutsche Keramische Gesellschaft (DKG). Edited by Yu-Ping Zeng, Shanghai Institute of Ceramics, Chinese Academy of Sciences, China.

  • Home
  • Early view
  • Articles
    • All articles
    • Recent Articles
    • Early Views
  • Issues
  • Submit an article
  • Guidelines for Referees
  • Guidelines for Authors
  • Open Access
  • Editorial Board
  • Copyright
  • Contact
  • Order journal / article
  • Customer area
  • Terms of Service

Journal Metrics

Web of science
Impact Factor: 1,220
Impact Factor without Journal Self Cites: 1,060
5 Year Impact Factor: 0,818

Scopus
Scimago Journal Rank (SJR):  0,378

 

Prices

Authors
1,300 € Open Access

Print Subscription
62 € per year

view all subscriptions

 

Payment methods

 Credit card

 Invoice

 Wire transfer

 

Articles

All articles  |  Recent articles

Influence of Phosphoric Acid Treatment on the Photocatalytic Activity of Zinc Oxide

H. Onoda, Y. Sato

Department of Informatics and Environmental Sciences, Kyoto Prefectural University, 1 – 5, Shimogamo Nakaragi-cyo, Sakyo-ku, Kyoto 606 – 8522, Japan

received August 12, 2016, received in revised form September 21, 2016, accepted October 12, 2016

Vol. 7, No. 4, Pages 397-402   DOI: 10.4416/JCST2016-00053

Abstract

Zinc oxide is often used as a white pigment for cosmetics; however, it exhibits photocatalytic activity that causes the decomposition of sebum on the skin when exposed to the ultraviolet radiation in sunlight. In this work, zinc oxide was reacted with various concentrations of phosphoric acid for several hours to synthesize a novel white pigment for cosmetics. The chemical composition, powder properties, photocatalytic activities, colors, and smoothness of these pigments were studied. The obtained materials exhibited x-ray diffraction peaks relating to zinc oxide and phosphate after phosphoric acid treatment. The ratio of zinc phosphate to zinc oxide was estimated from inductively coupled plasma results. The sample treated for 6 hours had a high P/Zn ratio, therefore this sample contained a larger amount of zinc phosphate. The concentration of phosphoric acid had less influence on the P/Zn ratio than the processing time. The particle size of the samples became larger with phosphoric acid treatment. The photocatalytic activity of the zinc oxide was inhibited by the phosphoric acid treatment. The obtained samples had enough high reflectance in the visible light region.

Download Full Article (PDF)

Keywords

Zinc oxide, phosphoric acid treatment, photocatalytic activity, particle size

References

1 Monteiro-Riviere, N.A., Wiench, K., Landsiedel, R., Schulte, S., Inman, A.O., Riviere, J.E.: Safety evaluation of sunscreen formulations containing titanium dioxide and zinc oxide nanoparticles in UVB sunburned skin: an in vivo study, Toxicol. Sci., 123, [1], 264 – 280, (2011).

2 Kajbafvala, A., Ghorbani, H., Paravar, A., Samberg, J.P., Kajbafvala, E., Sadrnezhaad, S.K.: Effects of morphology on photocatalytic performance of zinc oxide nanostructures synthesized by rapid microwave irradiation methods, Superlattice Mictrost., 51, [4], 512 – 522, (2012).

3 Nohynek, G.J., Dufour, E.K.: Nano-sized cosmetic formulations or solid nanoparticles in sunscreens: A risk to human health?, Arch. Toxicol., 86, 1063 – 1075, (2012).

4 Leite-Silva, V.R., Lamer, M.L., Sanchez, W.Y., Liu, D.C., Sanchez, W.H., Morrow, I., Martin, D., Silva, H.D.T., Prow, T.W., Grice, J.E., Roberts, M.S.: The effect of formulation on the penetration of coated and uncoated zinc oxide nanoparticles into the viable epidermis of human skin in vivo, Eur. J. Pharm. Biopharm., 84, [2], 297 – 308, (2013).

5 Weng, W., Otaibi, R.A., Alhumaimess, M., Conte, M., Bartley, J.K., Dummer, N.F., Hutchings, G.J., Kiely, C.J.: Controlling vanadium phosphate catalyst precursor morphology by adding alkane solvents in the reduction step of VOPO4·2H2O to VOHPO4·0.5H2O, J. Mater. Chem., 21, [40], 16136 – 16146, (2011).

6 Zhou, X., Bai, H., Ma, H., Li, H., Yuan, W., Du, H., Zhang, P., Xin, H.: Synthesis of zinc phosphate and zinc ammonium phosphate nanostructures with different morphologies through pH control, Mater. Charact., 108, 22 – 28, (2015).

7 Onoda, H., Funamoto, T.: Preparation and fluorescence properties of crystalline gel rare earth phosphates, J. Fluoresc., 25, [2], 247 – 251, (2015).

8 Onoda, H., Inagaki, Y., Kuwabara, A., Kitamura, N., Amezawa, K., Nakahira, A., Tanaka, I.: Synthesis and electrical conductivity of bulk tetra-valent cerium pyrophosphate, J. Ceram. Process. Res., 11, [3], 344 – 347, (2010).

9 Lee, Y., Schade, N.B., Sun, L., Fan, J.A., Bae, D.R., Mariscal, M.M., Lee, G., Capasso, F., Sacanna, S., Manoharan, V.N., Yi, G.: Ultrasmooth, highly spherical monocrystalline gold particles for precision plasmonics, ACS Nano, 7, [12], 11064 – 11070, (2013).

10 Kim, B.Y., Choi, J.W., Park, K.C., Youn, S.W.: Sebum, acne, skin elasticity, and gender difference – which is the major influencing factor for facial pores?, Skin Res. Tech., 19, [1], e45 – e53, (2011).

11 Yin, S., Minamidate, Y., Tonouchi, S., Goto, T., Dong, Q., Yamane, H., Sato, T., Solution synthesis of homogeneous plate-like multifunctional CeO2 particles, RSC Adv., 2, 5976 – 5982, (2012).

12 Onoda, H., Haruki, M., Toyama, T.: Preparation and powder properties of zinc phosphates with additives, Ceram. Intern., 40, [2], 3433 – 3438, (2014).

13 Onoda, H., Haruki, M., Toyama, T.: Influence of pH, concentration of sodium lactate as an additive and ultrasonic treatment on synthesis of zinc phosphate white pigments, Int. J. Cosmetic Sci., 36, [4], 321 – 326, (2014).

14 Eskizeybek, V., Sari, F., Gülce, H., Gülce, A., Avci, A.: Preparation of the new polyaniline/ZnO nanocomposite and its photocatalytic activity for degradation of methylene blue and malachite green dyes under UV and natural sun lights irradiations, Appl. Catal. B, 119 – 120, 197 – 206, (2012).

15 Lin, B., Li, X., Xu, B., Chen, Y., Gao, B., Fan, X.: Improved photocatalytic activity of anatase TiO2-pillared HTaWO6 for degradation of methylene blue, Microp. Mesop. Mater., 155, 16 – 23, (2012).

16 Xianjuan, L., Haiquan, X., Jing, C., Juncai, S., Yuxiang, Y., Xiangnong, L.: Research of Mica/Fe3O4 Pearlescent Pigment by Co-Precipitation, Glass Phys. Chem., 37, [3], 330 – 342, (2011).

Copyright

Göller Verlag GmbH

Special and Topcial Issues

Special Issue, 3/2025
Guest Editors:
Olaf Krause and Christian Dannert
Advances in Refractories

Topical Issue, 3/2017
Guest Editors:
Waltraud M. Kriven and Gregor J. G. Gluth
Geopolymers

Special Issue, 1/2017
Guest Editor:
Alexander Michaelis
6th International Congress on Ceramics (ICC6)

Topical Issue, 2/2016
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advan-ced steel technologies; A challenge for refractory materials and systems.

Topcial Issue, 4/2015
Low Temperature Co-fired Ceramics - LTCC

Topcial Issue, 2/2015
Status of Additive Manufacturing with Ceramics

Topical Focus, 4/2014
Materials Processing Science with Lasers as Energy Sources

Topical Issue, 2/2014
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advanced steel technologies; A challenge for refractory materials and systems.

Special Issue, 2/2013
Guest Editor:
Alexander Michaelis
Ceramic Materials and Components for Energy and Environmental Applications

Topical Issue, 1/2013
Ceramic Processing Science with Lasers as Energy Sources

Printed version

jcst 2015 02 cover

Order journal subscription
 

© 2009-2025 Göller Verlag GmbH