• Home
  • Contact
  • Login
  • Privacy
  • Imprint

Search

Journal of Ceramic Science and Technology

The Journal of Ceramic Science and Technology publishes original scientific articles on all topics of ceramic science and technology from all ceramic branches. The focus is on the scientific exploration of  the relationships between processing, microstructure and properties of sintered ceramic materials as well as on new processing routes for innovative ceramic materials. The papers may have either theoretical or experimental background. A high quality of publications will be guaranteed by a thorough double blind peer review process.

The Journal is published by Göller Verlag GmbH on behalf of the Deutsche Keramische Gesellschaft (DKG). Edited by Yu-Ping Zeng, Shanghai Institute of Ceramics, Chinese Academy of Sciences, China.

  • Home
  • Early view
  • Articles
    • All articles
    • Recent Articles
    • Early Views
  • Issues
  • Submit an article
  • Guidelines for Referees
  • Guidelines for Authors
  • Open Access
  • Editorial Board
  • Copyright
  • Contact
  • Order journal / article
  • Customer area
  • Terms of Service

Journal Metrics

Web of science
Impact Factor: 1,220
Impact Factor without Journal Self Cites: 1,060
5 Year Impact Factor: 0,818

Scopus
Scimago Journal Rank (SJR):  0,378

 

Prices

Authors
1,300 € Open Access

Print Subscription
62 € per year

view all subscriptions

 

Payment methods

 Credit card

 Invoice

 Wire transfer

 

Articles

All articles  |  Recent articles

Influence of the Chemical Composition of Ceramic Frits on the Kinetics of their Dissolution Process

A. Barba, J.C. Jarque, M. Orduña, M.F. Gazulla

Instituto de Tecnología Cerámica, Asociación de Investigación de las Industrias Cerámicas, Universitat Jaume I, Castellón, España.

received July 13, 2015, received in revised form September 2, 2015, accepted October 5, 2015

Vol. 7, No. 1, Pages 71-78   DOI: 10.4416/JCST2015-00034

Abstract

A study aboutof the influence of the chemical composition of frits ion the kinetics of their dissolution process has been performed, in order to haveobtain an more extensive knowledge about the solubility of different types of frits and to predict their behavior regarding to thewith regard to their dissolution process. The study has been conducted withusing four frits of the most usedfour of the frits most commonly used in the preparation of ceramic glazes: a zirconium white frit, a lead-containing boracic crystalline frit, a crystalline frit containing calcium and zinc and a sodium-containing boracic crystalline frit. The results have been fitted to a kinetic model in which the overall rate of the process is controlled by diffusion except the initial moments of the process, which are controlled by the chemical reaction. The differences inof solubility observed can be explained based onby the differences in the chemical composition of the frits. The kinetic model reproduces the experimental results using adjusting parameters that have physical meaning for the four studied frits.

Download Full Article (PDF)

Keywords

Frit solubility, glass-ceramics, kinetics, glazes,chemical durability

References

1 Barba, A., Jarque, J.C., Orduña, M., Gazulla M.F.: Kinetic model of the dissolution process of a zirconium white frit. influence of the temperature, J. Eur. Ceram. Soc., 35, 751 – 764, (2014).

2 Massera, J., Bourkhis, K., Petit, L., Couzi, M., Hupa, L., Hupa, H., Videau, J.J., Cardinal, T.: Effect of the glass composition on the chemical durability of zinc-phosphate-based glasses in aqueous solutions, J. Phys. Chem. Solids, 74, 121 – 127, (2013).

3 Nourmohammadi, J., Salarian, R., Solati-Hashjin, M., Moztarzadeh, F.: Dissolution behaviour and fluoride release from new glass composition used in glass ionomer cements, Ceram. Int., 33, 557 – 561, (2007).

4 Varila, L., Fagerlund, S., Lehtonen, T., Tuominen, J., Hupa, L.: Surface reactions of bioactive glasses in buffered solutions, J. Eur. Ceram. Soc., 32, 2757 – 2763, (2012).

5 Gin, S., Beaudoux, X., Angeli, F., Jégou, C., Godon, N.: Effect of composition on the short-term and long-term dissolution rates of ten borosilicate glasses of increasing complexity from 3 to 30 oxides, J. Non-Cryst. Solids, 358, 2559 – 2570, (2012).

6 Cailleteau, C., Weige, l.C., Ledieu, A., Barboux, P., Devreux, F.: On the effect of glass composition in the dissolution of glasses by water, J. Non-Cryst. Solids, 354, [2 – 9], 117 – 123, (2008).

7 Hernández Povedano, J.A., Oteo Mazo, J.L.: Reactions of glass surfaces with aqueous solutions, (in Spanish), Bol. Soc. Esp. Ceram. Vidr., 21, [2], 81 – 97, (1982).

8 Fernández Navarro, J.M.: El vidrio: constitución, fabricación y propiedades; 2nd edition. CSIC, Madrid, 1991

9 Strachan, D.M.: Glass dissolution: testing and modelling for long-term behaviour, J. Nucl. Mater., 298, 69 – 77, (2001).

10 Shinkareva, E.V., Bychko, G.V.: Chemical resistance of low-melting enamels for decorating glass products, Glass Ceram+, 62, 9 – 10, (2005).

11 Fröberg, L., Kronberg, T., Törnblom, S., Hupa, L.: Chemical durability of glazed surfaces, J. Eur. Ceram. Soc., 27, [2 – 3], 1811 – 1816, (2007).

12 Hupa, L., Bergman, R., Fröberg, L., Vane-Tempest, S., Hupa, M., Kronberg, T., Pesonen-Leinonen, E., Sjöberg A.M.: Chemical resistance and cleanability of glazed surfaces, Surf. Sci., 584, 113 – 118, (2005).

13 Sanmiguel, F., Ferrando, V., Amorós, J.L., Orts, M.J., Gazulla, M.F., Gómez M.P.: Solubilidad de fritas en suspensiones de esmaltes. Influencia de algunas variables de operación sobre la cinética del proceso, Técnica Cerámica, 275, 689 – 700, (1999).

14 Gómez-Tena, M.P., Bou, E., Moreno, A., Cook, S., Galindo, M.: Nueva materia prima borácica como componente de esmaltes cerámicos. Estudio de su solubilidad en suspensiones acuosas concentradas, Bol. Soc. Esp. Ceram. Vidr., 48, [1], 45 – 52, (2009).

15 Larena, M.T.: Solubilidad en medio acuoso de fritas cerámicas del sistema SiO2-PbO-B2O3. influencia de la composición química de la frita sobre su solubilidad a pH 7, Cerámica Información, 192, 10 – 19, (1993).

16 Huggins, M.L., Sun, K.H.: Calculation of density and optical constants of a glass from its composition in weight percentage, J. Am. Ceram. Soc., 26, [1], 4 – 11, (1943).

17 Gazulla, M.F., Barba, A., Orduña, M., Bautista, Y.: Stability of ceramic glaze compositions. Correlation between partial dissolution and rheological properties. Part I, Glass Technol.-Part A, 53, [3], 101 – 108, (2012).

18 Wen, C.Y.: Noncatalytic heterogeneous solid-fluid reaction models, Ind. Eng. Chem., 60, [9], 34 – 54, (1968).

19 Cable, M., Frade, J.R.: Diffusion controlled mass transfer to or from spheres with concentration-dependent diffusivity, Chem. Eng. Sci., 42, [11], 2525 – 2530, (1987).

20 Leturcq, G., Berger, G., Advocat, T., Fillet, C., Halgand, O., Vernaz, E.: Chemical durability of aluminosilicate glasses containing low solubility chemical elements, Mat. Res. Soc. Symp. Proc., 506, 199 – 206, (1998).

21 Dunken, H., Doremus, R.H.: Short time reactions of a Na2O-CaO-SiO2 glass with water and salt solutions, J. Non-Cryst. Solids, 92, 61 – 72, (1987).

22 Perera, G., Doremus, R.H.: Dissolution rates of silicate glasses in water at pH 7, J. Am. Ceram. Soc., 74, [6], 1269 – 1274, (1991).

Copyright

Göller Verlag GmbH

Special and Topcial Issues

Special Issue, 3/2025
Guest Editors:
Olaf Krause and Christian Dannert
Advances in Refractories

Topical Issue, 3/2017
Guest Editors:
Waltraud M. Kriven and Gregor J. G. Gluth
Geopolymers

Special Issue, 1/2017
Guest Editor:
Alexander Michaelis
6th International Congress on Ceramics (ICC6)

Topical Issue, 2/2016
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advan-ced steel technologies; A challenge for refractory materials and systems.

Topcial Issue, 4/2015
Low Temperature Co-fired Ceramics - LTCC

Topcial Issue, 2/2015
Status of Additive Manufacturing with Ceramics

Topical Focus, 4/2014
Materials Processing Science with Lasers as Energy Sources

Topical Issue, 2/2014
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advanced steel technologies; A challenge for refractory materials and systems.

Special Issue, 2/2013
Guest Editor:
Alexander Michaelis
Ceramic Materials and Components for Energy and Environmental Applications

Topical Issue, 1/2013
Ceramic Processing Science with Lasers as Energy Sources

Printed version

jcst 2015 02 cover

Order journal subscription
 

© 2009-2025 Göller Verlag GmbH