Hydrofluoric Acid versus Ytterbium Fiber Laser versus Argon Plasma Conditioning of Lithium Disilicate: Roughness, Topography, and Bond Strength Outcomes

H.Y. Aldryhim

Journal of Ceramic Science and Technology · Early View (advance online publication) (-1), pp. 1-8

DOI: 10.4416/JCST2026-00026

Download full article (PDF)

Abstract

To compare hydrofluoric acid (HFA), ytterbium fibre laser (YFL), and low-pressure argon plasma conditioning of lithium disilicate (LDS) ceramic on surface roughness (Ra), topography, and thermocycle micro-shear bond strength (μSBS), 60 LDS specimens were divided into four groups: untreated control, 9.5 % HFA, 1070-nm YFL, and argon plasma, each applied for 60 seconds. Five specimens per group underwent Ra profilometry and SEM analysis; the remaining ten received self-adhesive resin-cement cylinders, were stored, thermocycled, and tested for μSBS. Failure modes were classified after debonding. Ra and μSBS were analysed using one-way ANOVA with Tukey post hoc tests (α = 0.05). Ra differed significantly among groups (p < 0.05): control 0.51 ± 0.11 μm, HFA 1.23 ± 0.21 μm, YFL 1.30 ± 0.25 μm, plasma 0.57 ± 0.12 μm; HFA and YFL were comparable and significantly rougher than control and plasma, which did not differ. μSBS values were 6.69 ± 0.55, 9.45 ± 0.46, 9.48 ± 0.53, and 10.69 ± 0.31 MPa, respectively (p < 0.05), with plasma yielding the highest bond strength. Argon plasma achieved the greatest μSBS without increasing Ra, while HFA and YFL enhanced both roughness and bond strength comparably. Since bond strength was not associated with roughness, clinical protocol validation is warranted.

Keywords

Ceramics, dental bonding, hydrofluoric acid, lasers, solid-state, resin cements, surface properties