Manuscripts can be submitted via the Editorial Manager.

Journal of Ceramic Science and Technology | Early View

Advance online publication · articles published ahead of an issue

Lightweight Optimization of a Variable-Thickness Silicon Carbide Ceramic Impeller and Rotor-Dynamic Stability under High-Temperature and High-Speed Conditions

Xianfa Shen, Haiqiao Wang

Pages 1-14 · DOI: 10.4416/JCST2026-00014

A variable-thickness design strategy was developed for a pressureless-sintered silicon carbide ceramic impeller operating under coupled thermal and centrifugal loads. Eight impeller structures made from one common SiC composition were compared: an equal-thickness baseline, six gradient candidates, and a balanced optimum. A five-parameter B-spline thickness field was screened through 160 Latin-hypercube designs. Gaussian-process response surfaces and NSGA-II balanced mass, principal tensile stress, second critical speed, and aerodynamic loss; surrogate models were used for screening, whereas th …

Download PDF

Göller Verlag GmbH · info@goeller-verlag.de · Author Guidelines (PDF) · Site Notice · Privacy · Terms