Tianhong Chen, Tianhong Chen, Jun Fang, Jun Fang, Xue Yang, Mengying Fu, Xiang Gao
With the development of modern electronic technology toward miniaturization, integration, and high performance, functional electronic ceramics are being increasingly used in electronic packaging. However, the conventional high-temperature sintering of ceramics (typically > 1 200 °C) suffers from high energy consumption and incompatibility with low-cost metal electrodes, which severely limits their application in modern electronic devices. This review systematically summarizes recent advances in low-temperature sintering technologies for functional electronic ceramics. First, the fundamental mechanisms are discussed in terms of solid-state sintering, liquid-phase sintering, field-assisted sintering, and cold sintering. Second, design strategies for sintering aids based on low-melting-point glass phases and metal oxides are examined. Third, the principles and applications of advanced low-temperature sintering technologies, including cold sintering (
Functional electronic ceramics, low-temperature sintering, sintering aids, electronic packaging
Göller Verlag GmbH · info@goeller-verlag.de · Author Guidelines (PDF) · Site Notice · Privacy · Terms