Super-Translucent Multi-Layered Zirconia: Effects of Airborne-Particle Abrasion, Tribochemical Silica Coating, Zircos-E, and Atomic Layer Deposition of Silica Nanofilms on Roughness and Shear Bond Strength

R.S. Al-Hamdan

Journal of Ceramic Science and Technology · Early View (advance online publication) (-1), pp. 1-10

DOI: 10.4416/JCST2026-00019

Download full article (PDF)

Abstract

To compare four intaglio conditioning protocols – airborne-particle abrasion (APA), tribochemical silica coating (TBC), Zircos-E chemical etching, and atomic layer deposition of silica nanofilms (ALD-SiO2) – on surface roughness (Ra), topography, and shear bond strength (SBS) of super-translucent multi-layered (STML) zirconia luted with resin cement, 130 disc-shaped STML zirconia specimens were CAD/CAM-milled, sintered (1 550 °C), and allocated to five groups (n = 26): untreated control, APA (50 μm Al2O3), TBC, Zircos-E, and ALD-SiO2. Ra (contact profilometry, n = 8) and topography (SEM, n = 8) were assessed. Specimens were bonded with Panavia V5, thermocycled (10 000 cycles, 5 – 55 °C), and tested for SBS (n = 10) at 1.0 mm/min; failure modes were examined under stereomicroscopy (× 40). Data underwent one-way ANOVA with Tukey's HSD (p  0.05), while other groups exceeded control (p < 0.05). APA (13.85 ± 0.84 MPa) and ALD-SiO2 (14.34 ± 0.90 MPa) gave equivalent SBS despite different roughness (p > 0.05). TBC conferred the greatest Ra and SBS, followed by Zircos-E. Comparable APA and ALD-SiO2 bond strengths indicate chemical bonding can offset limited roughening. TBC and Zircos-E are clinically relevant strategies; clinical validation is warranted.

Keywords

Zirconia, tribochemical silica coating, atomic layer deposition, airborne-particle abrasion, shear bond strength, surface roughness