To evaluate the effect of hydrofluoric acid (HFA), sandblasting (SB), and Er,Cr:YSGG laser (ECL) conditioning on surface roughness topography, and repair bond strength (RBS) of composite resin bonded to two CAD/CAM hybrid ceramics. 156 discs (6 × 2 mm) were sectioned from Lava Ultimate (LU) and Cerasmart (CS) blocks (n = 78 each) and randomly allocated to three subgroups (n = 26): HFA-S (9.5 % HFA + silane), SB-S (50-µm Al2O3 + silane), and ECL-S (Er,Cr:YSGG + silane). Ra was measured by optical profilometry (ISO 4287:1997; n = 8) and topography by SEM (n = 8). Self-etch adhesive and nanohybrid composite were applied (n = 10/group), followed by 24-h storage in distilled water at 37 °C. RBS was tested at 1.0 mm/min, and failure modes were recorded stereomicroscopically (× 20). Data were analysed by one-way ANOVA with Tukey HSD post hoc test. ECL-S produced the highest Ra (LU 0.134 ± 0.03 µm; CS 0.098 ± 0.05 µm) and RBS (LU 11.54 ± 0.27 MPa; CS 10.12 ± 0.14 MPa). HFA-S yielded the lowest values in CS and SB-S the lowest in LU (all p 

Keywords

CAD/CAM, resin-matrix ceramic, lava ultimate, cerasmart, surface roughness, repair bond strength.