J. Zhijie, J. Zhijie, F. Shuai, L. Haiyan, B. Yiwan, Z. Cheng, W. Detian
In this work, we prepared mullite-zirconia/zirconia pre-stressed composites with excellent mechanical properties by means of pressureless sintering. Both the strength and toughness of zirconia could be significantly enhanced with the application of a pre-stressed coating. The optimal mechanical properties were obtained when the content of mullite in the coating was 40 wt%. The corresponding flexural strength and fracture toughness were 1250.48 ± 43.81 MPa and 12.39 ± 0.87 MPa·m1/2, an improvement of 39.15 % and 26.8 % compared with the values of zirconia, respectively. Basis for this reinforcement mechanism is that the achieved residual compressive stresses in the mullite-zirconia coating can simultaneously improve the strength and prevent crack propagation. The outstanding properties of mullite-zirconia/zirconia pre-stressed composites make these promising candidates for advanced manufacturing.
Pre-stressed strengthening, zirconia ceramics, mechanical properties, mullite
Göller Verlag GmbH · info@goeller-verlag.de · Author Guidelines (PDF) · Site Notice · Privacy · Terms