The Phase Composition and Mechanical Properties of Al2O3-TiN-TiC Ceramic Materials with Different Ni Content

Y. Fei, Ch. Huang, H. Liu

Journal of Ceramic Science and Technology, Vol. 10, No. 2 (2019), pp. 1-8

DOI: 10.4416/JCST2019-00012

Download full article (PDF)

Abstract

Research on the phase analysis of ceramic materials is less abundant than research on the microstructure. In this paper, Al2O3-TiN-TiC ceramic materials with different Ni content were fabricated by means of the hot-pressing technique. The effects of the content of Ni on the phase composition and the mechanical properties of sintered ceramic materials were investigated. The results showed that there were many diffraction peaks corresponding to the products of Ni in the range of 40°

Keywords

Al2O3-TiN-TiC ceramic, Ni content, phase composition, mechanical properties