E. Schwarzer, U. Scheithauer, M. Brosche, H.-J. Richter, T. Moritz
For the processing of ceramic green tapes to form 3D components, different technologies are known, for instance lamination to multilayer structures or folding. In the metals and plastics industries, deep drawing is, in addition to bending, a widely known method for reshaping sheet metals and polymers. This technology is not, however, applied for processing ceramic green tapes because of the downstream debinding and sintering steps. During the complex shaping process, the ceramic particles arranged within the polymer matrix become rearranged, which can result in inhomogeneous particle distribution. During sintering, this can lead to defects because of the resulting inhomogeneous shrinkage behavior. This study presents basic investigations into the deep drawing of ceramic green tapes. A special method was developed to investigate the particle distribution within the green tapes before and after the deep drawing and to correlate the results with the process conditions and the location of the investigated volume. One possible application for deep-drawn ceramic tapes could be as pre-product for non-planar kiln furniture. In combination with extruded pre-products, lamination, and co-sintering, large components with a low density and thermal mass can be produced with a top surface geometry similar to that of the sintered products.
Structural ceramic, tape casting, shaping, forming, deep drawing
Göller Verlag GmbH · info@goeller-verlag.de · Author Guidelines (PDF) · Site Notice · Privacy · Terms