Our website is currently undergoing maintenance. Article records and full texts remain available. Submissions can be made through the Editorial Manager.
Q. Wang, Q. Chang, K. Yang, Y. Wang, X. Wang, X. Li, J.-E. Zhou
Zircon-encapsulated carbon black is prepared as a black ceramic pigment by means of the sol-gel-spraying method. It is proposed that the dense zircon coating around the pigment is formed as a result of the fast transformation from sol into gel caused by the rapid extraction of solvent. To realize this, the preparation conditions are optimized as follows: the spray-drying temperature is 600 °C, the concentration of the ZrO2 sol is 0.8 mol/L, the mass ratio of the ethanol/water is 1:1, the mole ratio of the Si/Zr is 1.5 and the calcining conditions are 1250 °C with a holding time of 30 min. With these conditions, the chromatic value of the obtained pigment is L*=21.40, a*=-0.21, b*=-3.31. It is verified that the microstructure of tetragonal ZrO2 dispersed and distributed in amorphous SiO2 is necessary for the black ceramic pigment.
Ceramic pigment, zircon, encapsulated pigment, sol-gel-spraying
Göller Verlag GmbH · info@goeller-verlag.de · Site Notice · Privacy · Terms