F. Kern, V. Lindner, R. Gadow
In recent years, yttria-stabilized zirconia Y-TZP has attracted considerable interest in the field of dental restoration. However, the state-of-the-art Y-TZP materials made from coprecipitated powders only just comply with the current standard in terms of fracture resistance and grain size. In this study a new nanoscale starting powder produced with detonation synthesis was applied to produce a fully dense specimen by means of hot pressing in the sintering temperature range between 1250 – 1500 °C. Mechanical properties, microstructure and phase composition were studied. Low-temperature degradation behavior was quantified in an accelerated ageing test in a saturated water vapor at 134 °C. Between sintering temperatures of 1300 °C and1400 °C, the materials obtained show a combination of high strength > 1400 MPa, toughness of 6 MPa√m and fine grain size 90 % tetragonal phase up to ageing times of 10 h ≈ 35 years in vivo.
Zirconia, mechanical properties, phase composition, microstructure, low-temperature degradation
Göller Verlag GmbH · info@goeller-verlag.de · Author Guidelines (PDF) · Site Notice · Privacy · Terms