The Influence of Stabilizer Concentration on the Mechanical Properties of Alumina – 17 vol% Zirconia (0.6Y-2Y) Composites

F. Kern, S. Koummarasy, R. Gadow

Journal of Ceramic Science and Technology, Vol. 7, No. 3 (2016), pp. 295-300

DOI: 10.4416/JCST2016-00034

Download full article (PDF)

Abstract

Zirconia-toughened alumina (ZTA) with a zirconia content close to the percolation threshold has become the state-of-the art ceramic material for hip implants. In this study the stabilizer content in a ZTA with 17 vol% zirconia was varied between 0.6 – 2 mol% Y2O3 to understand more about the influence of the stabilizer concentration on mechanical properties, phase composition and formation of residual stress. It was found that fracture resistance reaches its maximum close to the stress neutral state where transformation stresses equilibrate residual cooling stresses while compressive stress in the alumina matrix favors higher strength.

Keywords

Ceramics, mechanical properties, zirconia, alumina, residual stress

Göller Verlag GmbH · info@goeller-verlag.de · Author Guidelines (PDF) · Site Notice · Privacy · Terms