Fabrication of MAX-Phase-Based Ceramics by Three-Dimensional Printing

Y. Ma, X. Yin, X. Fan, N. Travitzky, P. Greil

Journal of Ceramic Science and Technology, Vol. 6, No. 2 (2015), pp. 87-94

DOI: 10.4416/JCST2015-00006

Download full article (PDF)

Abstract

Three-dimensional printing (3DP) is a flexible and cost-effective method for direct digital manufacturing that provides capabilities for creating a wide range of part geometries in a broad variety of materials. Recently, a combined process of 3DP and reactive melt infiltration (RMI) has been applied to fabricate MAX-phase-based ceramics, exhibiting great potential in the fabrication of bulk compounds with complicated shape. This paper briefly summarizes the fabrication of Ti3AlC2- and Ti3SiC2-based ceramics with the combined process. 3DP facilitates the prior design of a porous preform with specific pore distribution and microstructure, which is beneficial to the control of the volume change of the following reaction in the RMI process, promoting the near-net-shape fabrication of MAX-phase-based ceramics with high flexibility in component geometry.

Keywords

Three-dimensional printing, RMI, Ti3SiC2, Ti3AlC2.

Göller Verlag GmbH · info@goeller-verlag.de · Author Guidelines (PDF) · Site Notice · Privacy · Terms