Manuscripts can be submitted via the Editorial Manager.

Crack Formation and Shape of Fracture Surface in Tabular-Alumina-Based Castables with Addition of Specific Aggregates

J. Schnieder, L. Lynen, N. Traon, T. Tonnesen, R. Telle

Journal of Ceramic Science and Technology, Vol. 5, No. 2 (2014), pp. 131-136

DOI: 10.4416/JCST2013-00039

Download full article (PDF)

Abstract

Understanding the mechanical fracture and the microstructural behavior of refractories subject to thermal shock treatment is fundamental for the design of high-performance refractory materials. In recent decades, understanding has been focused on mechanisms occurring at the crack tip, namely in advanced ceramics. The focus recently switched to phenomena occurring in a different process zone of the crack, the wake region or following process zone. To understand the mechanisms in this wake region, specific aggregates are used in a model castable formulation based on tabular alumina, namely eutectic aggregates composed of Al2O3-ZrO2-SiO2 and Al2O3-ZrO2. The influence of these aggregates on the elastic and thermo-mechanical properties as well as on the crack path and the fracture surface is examined. This survey will put emphasis on the impact of each aggregate on the fracture surface and the crack path after the model castable has undergone several thermal shock cycles.

Keywords

Refractories, microstructure analysis, eutectic aggregates, thermal shock