B. Eftekhari Yekta, Z. Hamnabard
The gradual addition of CaO to a SiO2-Al2O3-B2O3-MgO-K2O-F glass-ceramic composition led to the precipitation of gehlenite crystals and the formation of a potassium-calcium solid solution of fine mica crystals. The above additions almost tripled the bending strength and led to a ∼ 1.5-fold increase in the fracture toughness of the glass-ceramic specimens. When the amount of CaO reached 30 weight parts, the microhardness of glass-ceramic specimens was considerably reduced while their machinability was improved.