Our website is currently undergoing maintenance. Article records and full texts remain available. Submissions can be made through the Editorial Manager.

Submicrometer Silica Spheres Generated by Laser Fuming

C.M. Gomes, R. Müller, J. Günster, T. Mühler, R. Görke, J.G. Heinrich

Journal of Ceramic Science and Technology, Vol. 4, No. 1 (2013), pp. 11-18

DOI: 10.4416/JCST2012-00033

Download full article (PDF)

Abstract

The production of agglomerate-free SiO2 particles exhibiting a monomodal distribution of particle sizes of around 300 nm by means of direct laser fuming of micrometric SiO2 powders has been successfully demonstrated. With a 12 kW cw CO2 laser system, a production rate of up to 1 kilogram powder per hour was achieved. Almost ideal spherical amorphous SiO2 particles in a broad particle size distribution between 10 nm and several 100 nm (d50 ≈ 300 nm) were synthesized. Several observations suggest weak agglomeration forces between the particles. A temperature reduction of 200 °C for sintering powder compacts was observed.

Keywords

Laser, SiO2, nanopowder