J. Mucha, A. Chuchmała, D. Hreniak, A. Jeżowski, W. Strek
Thermal conductivity in transparent YAG nanoceramic was measured with the LTHP method in the temperature range 4 – 300 K. It was found that the thermal conductivity of nanoceramics with an average grains size of 16 nm was much lower compared to YAG crystal and polycrystalline ceramics composed of micro-size grains. The results were discussed in terms of the Kapitza resistance model. At about 200 K, Kapitza resistance becomes negative, which indicates a connection with apparent negative thermal conductivity.
Ceramics, amorphous materials, nanostructures, thermal conductivity, YAG