M.J. Pawar, S.S. Chaure, S.B. Deshmukh
The influence of cobalt doping on the densification and activation energy of Ce0.9Sm0.1O2-δ was studied. Solid solutions of Ce0.9-xCoxSm0.1O2-δ (x = 0, 0.05, 0.1 and 0.15) were prepared by means of a modified EDTA-glycol method. It was found that the degree of densification increases with an increasing concentration of cobalt. Almost full densification could be achieved at a sintering temperature of 1500 °C. The highest density (99.3 %) and minimum activation energy (0.81 eV) were observed for the composition Ce0.8Co0.1Sm0.1O2-δ.
SOFC; ceria; EDTA-glycol method; co-dopant; solid electrolytes