• Home
  • Contact
  • Login
  • Privacy
  • Imprint

Search

Journal of Ceramic Science and Technology

The Journal of Ceramic Science and Technology publishes original scientific articles on all topics of ceramic science and technology from all ceramic branches. The focus is on the scientific exploration of  the relationships between processing, microstructure and properties of sintered ceramic materials as well as on new processing routes for innovative ceramic materials. The papers may have either theoretical or experimental background. A high quality of publications will be guaranteed by a thorough double blind peer review process.

The Journal is published by Göller Verlag GmbH on behalf of the Deutsche Keramische Gesellschaft (DKG). Edited by Yu-Ping Zeng, Shanghai Institute of Ceramics, Chinese Academy of Sciences, China.

  • Home
  • Early view
  • Articles
  • Issues
    • All Issues
    • Recent issue
    • Early views
  • Submit an article
  • Guidelines for Referees
  • Guidelines for Authors
  • Open Access
  • Editorial Board
  • Copyright
  • Contact
  • Order journal / article
  • Customer area
  • Terms of Service

Journal Metrics

Web of science
Impact Factor: 1,220
Impact Factor without Journal Self Cites: 1,060
5 Year Impact Factor: 0,818

Scopus
Scimago Journal Rank (SJR):  0,378

 

Prices

Authors
1,300 € Open Access

Print Subscription
62 € per year

view all subscriptions

 

Payment methods

 Credit card

 Invoice

 Wire transfer

 

Issues

Recent Issue
 

Journal of Ceramic Science and Technology 2/2024

Vol. 15, No. 2

Original Articles

Source:
Journal of Ceramic Science and Technology

Comparison of Sintering Behavior of Silver, Aluminum and Copper Thick Films on Alumina Substrates using a Screen-Printing Method

J. Fang, T. Chen, Y. Jiao, Z. Zhang, S. Dong, Z. Huang

Vol. 15, No. 2, Pages 79-88   DOI: 10.4416/JCST2024-00007

Keywords: Sintering behavior, noble and base metal, thick films, screen printing

Abstract  |  References  |  Full Article

Source:
Journal of Ceramic Science and Technology

Reactive-Sintered Low-Thermal-Expansion Cordierite Ceramic with High Stiffness

Y. Guo, Y. Ge, W. Liu, J. Zhao, J. Zhang, S. Wang

Vol. 15, No. 2, Pages 69-78   DOI: 10.4416/JCST2024-00003

Keywords: Cordierite ceramics, reactive sintering. low coefficient of thermal expansion, phase evolution

Abstract  |  References  |  Full Article

Source:
Journal of Ceramic Science and Technology

MgO·nGa2O3 (n = 0.98 – 1.2) Transparent Ceramics with Longer Infrared Cut-Off Edge

W. Tao, D. Han, J. Zhang, Y. Shi, S. Wang

Vol. 15, No. 2, Pages 89-98   DOI: 10.4416/JCST2024-00009

Keywords: Magnesium gallate spinel, transparent ceramics, composition control, reactive sintering, microstructure evolution

Abstract  |  References  |  Full Article

Source:
Journal of Ceramic Science and Technology

Stress and Damage Analysis of the Innovative Brazing Seams between Al2O3 Ceramic and Nb Metal

F. Shi, B. Xu, X. Wang

Vol. 15, No. 2, Pages 55-68   DOI: 10.4416/JCST2024-00001

Keywords: Keywords: Ceramic-metal joints, brazing, residual stress, finite element method, ceramic damage

Abstract  |  References  |  Full Article

Special and Topcial Issues

Special Issue, 3/2025
Guest Editors:
Olaf Krause and Christian Dannert
Advances in Refractories

Topical Issue, 3/2017
Guest Editors:
Waltraud M. Kriven and Gregor J. G. Gluth
Geopolymers

Special Issue, 1/2017
Guest Editor:
Alexander Michaelis
6th International Congress on Ceramics (ICC6)

Topical Issue, 2/2016
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advan-ced steel technologies; A challenge for refractory materials and systems.

Topcial Issue, 4/2015
Low Temperature Co-fired Ceramics - LTCC

Topcial Issue, 2/2015
Status of Additive Manufacturing with Ceramics

Topical Focus, 4/2014
Materials Processing Science with Lasers as Energy Sources

Topical Issue, 2/2014
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advanced steel technologies; A challenge for refractory materials and systems.

Special Issue, 2/2013
Guest Editor:
Alexander Michaelis
Ceramic Materials and Components for Energy and Environmental Applications

Topical Issue, 1/2013
Ceramic Processing Science with Lasers as Energy Sources

Printed version

jcst 2015 02 cover

Order journal subscription
 

© 2009-2025 Göller Verlag GmbH