• Home
  • Contact
  • Login
  • Privacy
  • Imprint

Search

Journal of Ceramic Science and Technology

The Journal of Ceramic Science and Technology publishes original scientific articles on all topics of ceramic science and technology from all ceramic branches. The focus is on the scientific exploration of  the relationships between processing, microstructure and properties of sintered ceramic materials as well as on new processing routes for innovative ceramic materials. The papers may have either theoretical or experimental background. A high quality of publications will be guaranteed by a thorough double blind peer review process.

The Journal is published by Göller Verlag GmbH on behalf of the Deutsche Keramische Gesellschaft (DKG). Edited by Yu-Ping Zeng, Shanghai Institute of Ceramics, Chinese Academy of Sciences, China.

  • Home
  • Early view
  • Articles
  • Issues
    • All Issues
    • Recent issue
    • Early views
  • Submit an article
  • Guidelines for Referees
  • Guidelines for Authors
  • Open Access
  • Editorial Board
  • Copyright
  • Contact
  • Order journal / article
  • Customer area
  • Terms of Service

Journal Metrics

Web of science
Impact Factor: 1,220
Impact Factor without Journal Self Cites: 1,060
5 Year Impact Factor: 0,818

Scopus
Scimago Journal Rank (SJR):  0,378

 

Prices

Authors
1,300 € Open Access

Print Subscription
62 € per year

view all subscriptions

 

Payment methods

 Credit card

 Invoice

 Wire transfer

 

Issues

Recent Issue
 

Journal of Ceramic Science and Technology 1/2023

Vol. 14, No. 1

Original Articles

Source:
Journal of Ceramic Science and Technology

Characteristics and Sintering Behavior of (Hf-Ta-Ti-Zr-Nb)C High-Entropy Carbides Fabricated by High-Energy Ball Milling and Spark Plasma Sintering

J. Song, L.V. Duong, Ph.V. Trinh, N.N. Linh, D.D. Phuong, J. Seok, S.-Y. Kim, J. Han, H. Kim

Vol. 14, No. 1, Pages 17-24   DOI: 10.4416/JCST2022-00008

Keywords: High-entropy carbide, ultra-high-energy ball milling, spark plasma sintering

Abstract  |  References  |  Full Article

Source:
Journal of Ceramic Science and Technology

Investigation into the Solid-Solution (Na1-xKx)2Mo2O7 Ceramic and the Effect on Sintering Property

X. Yuan, H. Liu, Y. Wei, Y. Wang, Q. Gao

Vol. 14, No. 1, Pages 11-16   DOI: 10.4416/JCST2022-00006

Keywords: Low sintering temperature, sintering performance, dielectric ceramic

Abstract  |  References  |  Full Article

Source:
Journal of Ceramic Science and Technology

Glaze surface Defects causes and Prevention Controls

E. Youssef, N. Mostafa, J.E. Khoury, T. Merhej, R. Lteif

Vol. 14, No. 1, Pages 1-10   DOI: 10.4416/JCST2022-00003

Keywords: Ceramic, glaze defects, glaze pinholes, crawling, crazing

Abstract  |  References  |  Full Article

Source:
Journal of Ceramic Science and Technology

Synthesis, Phase Evolutions, and Properties of the Perovskite Ba6Ca2Ti2Nb3O19.5

Zh. Pan, H. Wei, J. Xu, L. Fang, X. Kuang

Vol. 14, No. 1, Pages 25-30   DOI: 10.4416/JCST2022-00013

Keywords: Ba6Ca2Ti2Nb3O19.5, simple cubic perovskite, B-site disorder, high permittivity, alternating current impedance.

Abstract  |  References  |  Full Article

Source:
Journal of Ceramic Science and Technology

High-Performance, Corrosion-Resistance Sealing Glasses for Primary Lithium Batteries: Preparation, Properties and Applications

Z. Wang, S.J. Hua, W.H. Liu, W.B. Yang, Q. Feng

Vol. 14, No. 1, Pages 31-38   DOI: 10.4416/JCST2022-00015

Keywords: Glass, sealing, performance, corrosion resistance.

Abstract  |  References  |  Full Article

Source:
Journal of Ceramic Science and Technology

Sintering and High-Temperature Strength of (Ti,Hf,Ta)C Medium-Entropy Ceramics Consolidated by Biphasic Carbide Powders

F.L. Qin, X.G. Wang, X.F. Wang, Q.Q. Yang, R.Z. Li, W. Gao, C. Zhang, D.Y. Jiang

Vol. 14, No. 1, Pages 39-48   DOI: 10.4416/JCST2023-00002

Keywords: Medium-entropy ceramics (Ti,Hf,Ta)C, sluggish diffusion effect, high-temperature flexural strength.

Abstract  |  References  |  Full Article

Special and Topcial Issues

Special Issue, 3/2025
Guest Editors:
Olaf Krause and Christian Dannert
Advances in Refractories

Topical Issue, 3/2017
Guest Editors:
Waltraud M. Kriven and Gregor J. G. Gluth
Geopolymers

Special Issue, 1/2017
Guest Editor:
Alexander Michaelis
6th International Congress on Ceramics (ICC6)

Topical Issue, 2/2016
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advan-ced steel technologies; A challenge for refractory materials and systems.

Topcial Issue, 4/2015
Low Temperature Co-fired Ceramics - LTCC

Topcial Issue, 2/2015
Status of Additive Manufacturing with Ceramics

Topical Focus, 4/2014
Materials Processing Science with Lasers as Energy Sources

Topical Issue, 2/2014
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advanced steel technologies; A challenge for refractory materials and systems.

Special Issue, 2/2013
Guest Editor:
Alexander Michaelis
Ceramic Materials and Components for Energy and Environmental Applications

Topical Issue, 1/2013
Ceramic Processing Science with Lasers as Energy Sources

Printed version

jcst 2015 02 cover

Order journal subscription
 

© 2009-2025 Göller Verlag GmbH