Journal of Ceramic Science and Technology

The Journal of Ceramic Science and Technology publishes original scientific articles on all topics of ceramic science and technology from all ceramic branches. The focus is on the scientific exploration of  the relationships between processing, microstructure and properties of sintered ceramic materials as well as on new processing routes for innovative ceramic materials. The papers may have either theoretical or experimental background. A high quality of publications will be guaranteed by a thorough double blind peer review process.

The Journal is published by Göller Verlag GmbH on behalf of the Deutsche Keramische Gesellschaft (DKG). Edited by Yu-Ping Zeng, Shanghai Institute of Ceramics, Chinese Academy of Sciences, China.

  • Home
  • Early view
  • Articles
    • All articles
    • Recent Articles
    • Early Views
  • Issues
  • Submit an article
  • Guidelines for Referees
  • Guidelines for Authors
  • Open Access
  • Editorial Board
  • Copyright
  • Contact
  • Order journal / article
  • Customer area
  • Terms of Service

Journal Metrics

Web of science
Impact Factor: 1,220
Impact Factor without Journal Self Cites: 1,060
5 Year Impact Factor: 0,818

Scopus
Scimago Journal Rank (SJR):  0,378

 

Prices

Authors
1,300 € Open Access

Print Subscription
62 € per year

view all subscriptions

 

Payment methods

 Credit card

 Invoice

 Wire transfer

 

Articles

All articles  |  Recent articles

Impact of Lithium Disilicate Ceramic Surface Modifiers and Resin Cement of Different Viscosities on Surface Roughness and Bond Strength after Artificial Aging: A SEM Assessment

A. Alshahrani1, R.S. Alhamdan2, R.T. Alsaqat3, S. Alresayes1, M. Q Al Rifaiy1, B. Almutairi2

1 Department of Prosthetic Dental Sciences, College of Dentistry, King Saud University, Riyadh, Saudi Arabia.
2 Department of Restorative Dental Science, College of Dentistry, King Saud University, Riyadh 11545, Saudi Arabia.
3 General Practitioner, King Abdullah University Hospital, Princess Noura Bint Abdulrahman University, Dental Clinic department, Restorative division.

received November 13, 2024, received in revised form November 21, 2024, accepted November 25, 2024

Vol. 16, No. 1, Pages 37-44   DOI: 10.4416/JCST2024-00028

Abstract

The impact of ceramic surface conditioners and resin cement with different viscosities on the surface roughness (Ra) and strength of the bond of dentin to lithium disilicate ceramics (LDC) at baseline and after aging has been investigated. Dentin and LDC discs were prepared. The discs were conditioned. Group 1: HFA+S, Group 2: SECP and Group 3: Er, Cr: YSGG. Ra and topographic analysis of conditioned discs was performed. Based on high and low viscosities, conditioned discs were bonded with dentin. Bonded samples with low and high viscosity underwent aging while others were not aged. SBS testing with a UTM machine was performed on both aged and non-aged samples and failure analysis was conducted. The means and SD for the SBS and Ra were analyzed using a one-way ANOVA and the Tukey post hoc tests. The maximum Ra score was obtained in specimens conditioned with HF acid-S. Group-2 samples (SECP) displayed the minimum value for Ra. The highest SBS values were attained by Group 1A (HF(S)+High) samples at baseline. The lowest SBS scores were presented by Group 2A (SECP+High) samples after thermal aging. The SBS of LDC is influenced by their microstructure obtained after surface conditioning. Long-term thermal aging causes a decrease in the mechanical performance of LDC discs bonded to dentin using high-viscosity resin cement.

Download Full Article (PDF)

Keywords

Lithium disilicate ceramics, viscosity, thermal aging, surface modification

References

1 McLean, J.W., Odont, D.: Evolution of dental ceramics in the twentieth century, J. Prosthet. Dent. [Internet], 85, [1], 61 – 66, (2001).

2 Kumbuloglu, O., Lassila, L.V.J., User, A, Toksavul, S., Vallittu, P.K.: Shear bond strength of composite resin cements to lithium disilicate ceramics, J. Oral Rehabil., 32, [2], 128 – 133, (2005).

3 Albaker, A.M., Al Deeb, L., Alhenaki, A.M. et al.: Bonding integrity and compressive strength of re-bonded, surface conditioned and er cr YSGG laser treated lithium disilicate ceramics, J. Appl. Biomater. Funct. Mater., 18, (2020).

4 Ellakany, P., Madi, M., Aly, N.M., Alshehri, T., Alameer, S.T., Al-Harbi, F.A.: Influences of different CAD/CAM ceramic compositions and thicknesses on the mechanical properties of ceramic Restorations: an In Vitro study, Materials (Basel).16, [2], 646 (2023).

5 Alkhudhairy, F., Naseem, M., Ahmad, Z.H., Alnooh, A.N., Vohra, F.: Efficacy of phototherapy with different conventional surface treatments on adhesive quality of lithium disilicate ceramics, Photodiagnosis Photodyn. Ther., 25, 292 – 295, (2019).

6 Bitencourt, S., Piacenza, L.T., Souza, J.P.D.V., et al.: The effect of different plasma treatments on the surface properties and bond strength between lithium disilicate and resin cement, J. Adhes. Dent., 22, [5], (2020).

7 Lee, M.H., Son, J.S., Kim, K.H., Kwon, T.Y.: Improved resin-zirconia bonding by room temperature hydrofluoric acid etching, Materials (Basel)., 8, [3], 850 – 866, (2015).

8 Han, A, Tsoi, J.K.H., Matinlinna, J.P., Chen, Z.: Influence of grit-blasting and hydrofluoric acid etching treatment on surface characteristics and biofilm formation on zirconia, Coatings, 7, [8], 130, (2017).

9 Flamant, Q., García Marro, F., Roa Rovira, J.J., Anglada, M.: Hydrofluoric acid etching of dental zirconia. part 1: etching mechanism and surface characterization, J. Eur. Ceram. Soc., 36, [1], 121 – 134, (2016).

10 Tsujimoto, A., Shimatani, Y., Nojiri, K, et al.: Influence of surface wetness on bonding effectiveness of universal adhesives in etch-and-rinse mode, Eur. J. Oral Sci., 127, [2], 162 – 169, (2019).

11 Al Ahdal, K., Maawadh, A.M., Al Deeb, L., Alshamrani, A.S., Almohareb, T., Alrahlah, A.: Effect of malachite green, ocimum sanctum, and er, Cr: YSGG laser on antimicrobial activity against S.mutans and CAD disinfection bonded to resin restoration, Photodiagnosis Photodyn. Ther., 42, (2023).

12 Alkhudhairy, F., AlKheraif, A., Bin-Shuwaish, M., Al-Johany, S., Naseem, M., Fahim Vohra Mc.: Effect of er,Cr:YSGG laser and ascorbic acid on the bond strength and microleakage of bleached enamel surface, Photomed. Laser Surg., XX, [Xx], 1 – 8 (2018).

13 Albalawi. F.S.: Efficacy of er, Cr: YSGG laser phosphoric acid gel and riboflavin activated by photodynamic therapy on enamel reconditioning rebonded to metallic brackets: an invitro study, Photodiagnosis Photodyn. Ther., 40, (2022).

14 Gonzaga, C.C., Cesar, P.F., Miranda, W.G., Yoshimura, H.N.: Slow crack growth and reliability of dental ceramics, Dent. Mater., 27, [4], 394 – 406 (2011).

15 Dapieve, K.S., Velho, H.C,, da Rosa, L.S., et al.: Ceramic surface conditioning, resin cement viscosity, and aging relationships affect the load-bearing capacity under fatigue of bonded glass-ceramics, J. Mech. Behav. Biomed. Mater., 139, (2023).

16 Barbon, F.J., Moraes, R.R., Isolan, C.P., Spazzin, A.O., Boscato, N.: Influence of inorganic filler content of resin luting agents and use of adhesive on the performance of bonded ceramic, J. Prosthet. Dent., 122, [6], 566.e1 – 566.e11, (2019).

17 Dapieve, K.S., Machry, R.V., Cadore-Rodrigues, A.C., et al.: Cyclic fatigue vs static loading for shear bond strength test of lithium disilicate and dentin substrates: A comparison of resin cement viscosities, Dent. Mater., 38, [12], 1910 – 1920, (2022).

18 Dapieve, K.S., Velho, H.C., da Rosa, L.S., et al.: Ceramic surface conditioning, resin cement viscosity, and aging relationships affect the load-bearing capacity under fatigue of bonded glass-ceramics, J. Mech. Behav. Biomed. Mater., 139, 105667, (2023).

19 Alatawi, R.A.S., Elsayed, N.H., Mohamed, W.S.: Influence of hydroxyapatite nanoparticles on the properties of glass ionomer cement, J. Mater. Res. Technol., 8, [1], 344 – 349, (2019).

20 Andreatta Filho, O.D., Araújo, M.A.J. de, Bottino, M.A., Nishioka, R.S., Menezes, M.M.: Study of thermocycling effect on the bond strength between an aluminous ceramic and a resin cement, J. Appl. Oral Sci., 13, [1], 53 – 57, (2005).

21 Vechiato Filho, A.J., Dos Santos, D.M., Goiato, M.C., et al.: Surface characterization of lithium disilicate ceramic after nonthermal plasma treatment, J. Prosthet. Dent., 112, [5], 1156 – 1163, (2014).

22 Tarek, M., Mosleh, I,, Zaghloul, H.: Effect of er,Cr:YSGG laser versus acid etching surface treatment on the surface roughness and topography of two pressable lithium disilicate Ceramics. „In-Vitro Study”, Egypt. Dent. J., 67, [2], 1571 – 1581, (2021).

23 Sundfeld Neto, D., Naves, L.Z., Costa, A.R., et al.: The effect of hydrofluoric acid concentration on the bond strength and morphology of the surface and interface of glass ceramics to a resin cement, Oper. Dent., 40, [5], 470 – 479, (2015).

24 Yilmaz-Savas, T., Demir, N., Ozturk, A.N., Kilic, H.S.: Effect of different surface treatments on the bond strength of lithium disilicate ceramic to the zirconia core, Photomed. Laser Surg., 34, [6], 236 – 243, (2016).

25 Cuzic, C., Jivanescu, A., Negru, R.M., Hulka, I., Rominu, M.: The influence of hydrofluoric acid temperature and application technique on ceramic surface texture and shear bond strength of an adhesive cement, Materials (Basel)., 16, [12], (2023).

26 Moreira, P., Review GC-DS, 2024 U: Effect of hydrofluoric acid and self-etch ceramic primers on the flexural strength and fatigue resistance of glass ceramics: A systematic review and meta, ElsevierPM Moreira, GLM Carvalho, R Castro Albuquerque, CB AndréJapanese Dent. Sci. Rev. (2024).

27 Tribst, J.P.M., Monteiro, J.B., Venturini, A.B., et al.: Fatigue failure load of resin-bonded simplified lithium disilicate glass-ceramic restorations: Effect of ceramic conditioning methods, J. Adhes. Dent., 21, [4], (2019).

28 Lopes, G.C., Perdigão, J., Baptista, D., Ballarin, A.: Does a self-etching ceramic primer improve bonding to lithium disilicate ceramics? Bond strengths and FeSEM analyses. Oper. Dent., 44, [2], 210 – 218, (2019).

29 Alrahlah, A, Awad, M.M., Vohra, F., Al-Mudahi, A., Al jeaidi, Z.A., Elsharawy, M.: Effect of self etching ceramic primer and universal adhesive on bond strength of lithium disilicate ceramic, J. Adhes. Sci. Technol., 31, [23], 2611 – 2619, (2017).

30 Dapieve, K.S., Pereira, G.K.R., Venturini, A.B., et al.: Do resin cement viscosity and ceramic surface etching influence the fatigue performance of bonded lithium disilicate glass-ceramic crowns? Dent. Mater., 38, [3], e59 – e67, (2022).

31 Attia, A, Kern, M.: Influence of cyclic loading and luting agents on the fracture load of two all-ceramic crown systems, J. Prosthet. Dent., 92, [6], 551 – 556, (2004).

32 Niem, T., Youssef, N., Wöstmann, B.: Influence of accelerated ageing on the physical properties of CAD/CAM restorative materials, Clin. Oral Investig., 24, [7], 2415 – 2425 (2020).

Copyright

Göller Verlag GmbH

Special and Topcial Issues

Special Issue, 3/2025
Guest Editors:
Olaf Krause and Christian Dannert
Advances in Refractories

Topical Issue, 3/2017
Guest Editors:
Waltraud M. Kriven and Gregor J. G. Gluth
Geopolymers

Special Issue, 1/2017
Guest Editor:
Alexander Michaelis
6th International Congress on Ceramics (ICC6)

Topical Issue, 2/2016
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advan-ced steel technologies; A challenge for refractory materials and systems.

Topcial Issue, 4/2015
Low Temperature Co-fired Ceramics - LTCC

Topcial Issue, 2/2015
Status of Additive Manufacturing with Ceramics

Topical Focus, 4/2014
Materials Processing Science with Lasers as Energy Sources

Topical Issue, 2/2014
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advanced steel technologies; A challenge for refractory materials and systems.

Special Issue, 2/2013
Guest Editor:
Alexander Michaelis
Ceramic Materials and Components for Energy and Environmental Applications

Topical Issue, 1/2013
Ceramic Processing Science with Lasers as Energy Sources

Printed version

jcst 2015 02 cover

Order journal subscription
 

© 2009-2025 Göller Verlag GmbH