Synthesis, Phase Evolutions, and Properties of the Perovskite Ba6Ca2Ti2Nb3O19.5
Zh. Pan, H. Wei, J. Xu, L. Fang, X. Kuang
MOE Key Laboratory of New Processing Technology for Nonferrous Metal and Materials; Guangxi Universities Key Laboratory of Non-ferrous Metal Oxide Electronic Functional Materials and Devices; College of Materials Science and Engineering, Guilin University of Technology, Guilin 541004, P. R. China
received December 16, 2022, received in revised form Febuary 2, 2023, accepted Febuary 2, 2023
Vol. 14, No. 1, Pages 25-30 DOI: 10.4416/JCST2022-00013
Abstract
In the present study, Ba6Ca2Ti2Nb2+xO17+2.5x (BCTN, x ≤ 1.0) materials were synthesized with the traditional solid-state reaction method. The phase evolution, structure, relative permittivity, and electrical conduction properties of these materials were studied. The results revealed that increasing the Nb content and improving the calcining temperature favored the formation of a pure simple cubic perovskite structure. For the end member of Ba6Ca2Ti2Nb2+xO17+2.5x, i.e. Ba6Ca2Ti2Nb3O19.5, Rietveld structural refinement disclosed that about 25 % Ca ions and all the Ba ions occupied the A site, while the remaining cations were disordered and occupied the B site. Thus, it can also be written as (Ba6Ca0.5)(Ca1.5Ti2Nb3)O19.5. This material exhibited high permittivity up to 80 and the electrical conductivity was 1.33×10-4 S/cm at 800 °C which was dominated by electronic conduction.
Download Full Article (PDF)
Keywords
Ba6Ca2Ti2Nb3O19.5, simple cubic perovskite, B-site disorder, high permittivity, alternating current impedance.
References
1 Kuang, X.-J., Price, T., Iddles, D.M., Rosseinsky, M.J.: Isolation of two-dimensional 2:1 cation-ordered perovskite units by anion vacancy ordering in Ba6Na2Nb2P2O17, Inorg. Chem., 47, [19], 8444 – 50, (2008).
2 Kaletsch, A., Bezold, A., Pfaff, E.M., Broeckmann, C.: Effect of copper oxide content in AgCuO braze alloy on microstructure and mechanical properties of reactive-air-brazed Ba0.5Sr0.5Co0.8Fe0.2O3(BSCF), J. Ceram. Sci. Technol., 03, [02], 95 – 104, (2012).
3 Jancar, B., Suvorov, D., Valant, M., Drazic, G.: Characterization of CaTiO3-NdAlO3 dielectric ceramics, J. Eur. Ceram. Soc., 23, [9], 1391 – 400, (2003).
4 Kuang, X.-J., Allix, M.M.B., Claridge, J.B., Niu, H.-J., Rosseinsky, M.J, Ibberson, R.M., Iddles, D.M.: Crystal structure, microwave dielectric properties and AC conductivity of B-cation deficient hexagonal perovskites La5MxTi4-xO15 (x = 0.5, 1; M = Zn, Mg, Ga, Al), J. Mater. Chem., 16, [11], 1038, (2006).
5 Davies, P.K.: Cation ordering in complex oxides, Curr. Opin. Solid State Mater. Sci., 4, 467 – 71, (1999).
6 Liu, Y., Huang, X.: High permittivity and dielectric response of CaCu3Ti3.9(Y0.5Nb0.5)0.1O12 Ceramics, J. Ceram. Sci. Technol., 08, [2], 243 – 48, (2017).
7 Huang, Y.-H., Karppinen, M., Yamauchi, H., Goodenough, J.B.: Systematic studies on effects of cationic ordering on structural and magnetic properties in Sr2FeMoO6, Phys Rev. B., 73, [10], 104408 – 1-5, (2006).
8 Rodgers, J.A., Battle, P.D., Dupre, N., Grey, C.P., Sloan, J.: Cation and spin ordering in the n =1 ruddlesden-popper phase La2Sr2LiRuO8, Chem. Mater., 16, [22], 4257 – 66, (2004).
9 Millange, F., Caignaert, V., Domenges, C., Raveau, B.: Order-disorder phenomena in new LaBaMn2O6-x CMR perovskites crystal and magnetic structure, Chem. Mater., 10, [7], 1974 – 83, (1998).
10 Kim, S.W.G., Jacobson, A.J.: Oxygen exchange kinetics of epitaxial PrBaCo2O5 thin films, Appl. Phys. Lett., 88, [24103], 1 – 3, (2006).
11 Harada, Y.H., Hirakoso, Y.J., Kawai, H., Kuwano, J.: Order-disorder of the A-site ions and lithium ion conductivity in the perovskite solid solution La0.67-xLi3xTiO3 (x= 0.11), Solid State Ionics, 121, 245 – 51, (1999).
12 Thirumal, M., Davies, P.K.: Ba8ZnTa6O24: A new high q dielectric perovskite, J. Am. Ceram. Soc, 88, [8], 2126 – 28, (2005).
13 Surendran, K.P., Sebastian, M.T.: Low loss dielectrics in Ba[(Mg1/3Ta2/3)1-xTix]O3 and Ba[(Mg1-xZnx)1/3Ta2/3]O3 systems, J. Mater. Res., 20, [11], 2919 – 26, (2005).
14 Rietveld, H.M.: A profile refinement method for nuclear and magnetic structures, J. Appl. Cryst., 2, [65], 65 – 71, (1969).
15 Irvine, T.S., Sinclair, D.C., West, A.R.: Electroceramics characterization by impedance spectroscopy, Adv. Mater., 2, [3], 132 – 38, (1990).
Copyright
Göller Verlag GmbH