The Interaction of Stacking Faults and the Doping of Si in TiC
Q. Liu, F.G. Qi, X.L. Wang, H.M. Ding, Y. Shi
School of Energy Power and Mechanical Engineering, North China Electric Power University, Baoding 071003, PR China
received April 26, 2017, received in revised form May 21, 2017, accepted June 2, 2017
Vol. 8, No. 4, Pages 493-498 DOI: 10.4416/JCST2017-00027
Abstract
In this work, the interaction of stacking faults and the doping of Si in TiC has been studied. It has been found that the SFs and doping of Si influence each other, but the effect is limited. However, both of them are closely related to the carbon vacancies. It is considered that the carbon vacancies simultaneously promote the formation of SFs and the doping of Si, and then the doped Si and carbon vacancies tend to segregate in the SF layers, which can result in the formation of Ti3SiC2 platelets. And the segregation process can be enhanced by their easier diffusion in the SF layers.
Download Full Article (PDF)
Keywords
Defects, ceramic, vacancies, simulation.
References
1 Miriyev, A., Sinder, M., Frage, N.: Thermal stability and growth kinetics of the interfacial TiC layer in the ti alloy/carbon steel system, Acta Mater., 75, 348 – 355, (2014).
2 Zhang, Y., Xiao. G., Xu, C., Yi, M., Meng, X.: Anisotropic fracture toughness and microstructure of graphene-reinforced TiC/Si3N4 composite, J. Ceram. Sci. Tech., 4, 323 – 327, (2016).
3 Zhou, M.Y., Rodrigo, P.D.D., Wang, X.J., Hu, J.B., Dong, S.M., Cheng, Y.B.: A novel approach for preparation of dense TiC-SiC nanocomposites by sol-gel infiltration and spark plasma sintering, J. Eur. Ceram. Soc., 34, 1949 – 1954, (2014).
4 Yu, R., Zhan, Q., He, L.L., Zhou, Y.C., Ye, H.Q.: Si-induced twinning of TiC and formation of Ti3SiC2 platelets, Acta Mater., 50, 4127 – 4135, (2002).
5 Yu, R., He, L.L., Ye, H.Q.: Effects of Si and Al on twin boundary energy of TiC, Acta Mater., 51, 2477 – 2484, (2003).
6 Zhou, C.L., Ngai, T.W.L., Lu, L., Li, Y.Y.: Fabrication and characterization of pure porous Ti3SiC2 with controlled porosity and pore features, Mater. Lett., 131, 280 – 283, (2014).
7 Istomin, P., Nadutkin, A., Grass, V.: Fabrication of Ti3SiC2-based ceramic matrix composites by a powder-free SHS technique, Ceram. Int., 39, 3663 – 3667, (2013).
8 Johansson, L.I.: Electronic and structural properties of transition-metal carbide and nitride surfaces, Surf. Sci. Rep., 21,177 – 250, (1995).
9 Govind, N., Petersen, M., Fitzgerald, G., King-Smith, D., Andzelm, J.: A generalized synchronous transit method for transition state location, Comput. Mater. Sci., 28, 250 – 258, (2003).
10 Music, D., Riley, D.P., Schneider, J.M.: Energetics of point defects in TiC, J. Eur. Ceram. Soc., 29, 773 – 777, (2009).
11 Zhang, P., Nie, J.F., Gao, T., Wang, T., Liu, X.F.: Influence of nitrogen on the synthesis and nucleation ability of TiCx in Al-Ti-C master alloy, J. Alloy. Compd. 601, 267 – 273, (2014).
12 Tsetseris, L., Pantelides, S.T.: Vacancies, interstitials and their complexes in titanium carbide, Acta Mater., 56, 2864 – 2871, (2008).
13 Guemmaz, M., Mosser, A., Parlebasb, J.C.: Electronic changes induced by vacancies on spectral and elastic properties of titanium carbides and nitrides, J. Electron Spectrosc., 107, 91 – 101, (2000).
14 Hugosson, H.W., Korzhavyi, P., Jansson, U., Johansson, B., Eriksson, O.: Phase stabilities and structural relaxations in substoichiometric TiC1-x, Phys. Rev. B, 63, 165116 – 165123, (2001).
15 Ding, H.M., Fan, X.L., Chu, K.Y., Zhang, X.C., Liu, X.F.: The influence of carbon vacancies on the stacking fault energy of TiC, J. Eur. Ceram. Soc., 34, 1893 – 1897, (2014).
16 Li, X.X., Xiang, J.Y., Hu, W.T.: {111} twinning structure and interfacial energy in nonstoichiometric TiCx with ordered carbon vacancies, Mater. Charac., 90, 94 – 98, (2014).
17 Tsurekawa, S., Yoshinaga, H.: Dislocation dissociation in titanium carbide crystal, J. Japan Inst. Metals, 58, 390 – 396, (1994).
18 Bursik, J.: Ordering of substoichiometric δ-TiCx phase in Ti-V-C alloys, Phys. Stat. Sol. A, 174, 327 – 335, (1999).
19 Barsoum, M.W.: The MN+1AXN phases: A new class of solids, Prog. Solid State Chem., 28, 201 – 281, (2000).
20 Price, D.L., Cooper, B.R.: Total energies and bonding for crystallographic structures in titanium-carbon and tungsten-carbon systems, Phys. Rev. B, 39, 4945 – 4957, (1989).
21 Dridi, Z., Bouhafs, B., Ruterana, P., Aourag, H.: First-principles calculations of vacancy effects on structural and electronic properties of TiCx and TiNx, J. Phys.: Condens. Matter, 14, 10237 – 10249, (2002).
Copyright
Göller Verlag GmbH