Journal of Ceramic Science and Technology

The Journal of Ceramic Science and Technology publishes original scientific articles on all topics of ceramic science and technology from all ceramic branches. The focus is on the scientific exploration of  the relationships between processing, microstructure and properties of sintered ceramic materials as well as on new processing routes for innovative ceramic materials. The papers may have either theoretical or experimental background. A high quality of publications will be guaranteed by a thorough double blind peer review process.

The Journal is published by Göller Verlag GmbH on behalf of the Deutsche Keramische Gesellschaft (DKG). Edited by Yu-Ping Zeng, Shanghai Institute of Ceramics, Chinese Academy of Sciences, China.

  • Home
  • Early view
  • Articles
    • All articles
    • Recent Articles
    • Early Views
  • Issues
  • Submit an article
  • Guidelines for Referees
  • Guidelines for Authors
  • Open Access
  • Editorial Board
  • Copyright
  • Contact
  • Order journal / article
  • Customer area
  • Terms of Service

Journal Metrics

Web of science
Impact Factor: 1,220
Impact Factor without Journal Self Cites: 1,060
5 Year Impact Factor: 0,818

Scopus
Scimago Journal Rank (SJR):  0,378

 

Prices

Authors
1,300 € Open Access

Print Subscription
62 € per year

view all subscriptions

 

Payment methods

 Credit card

 Invoice

 Wire transfer

 

Articles

All articles  |  Recent articles

Synthesis of Calcium Hexaboride Powder via Boro/Carbothermal Reduction with a Gel Precursor

D. Yilmaz Çakta1, N. Koç1, S. Turan2

1 Department of Metallurgy and Materials Engineering, Eskisehir Osmangazi University, Eskisehir, Turkey.
2 Department of Materials Science and Engineering, Anadolu University, Eskisehir, Turkey.

received June 13, 2016, received in revised form July 25, 2016, accepted September 8, 2016

Vol. 7, No. 4, Pages 349-356   DOI: 10.4416/JCST2016-00044

Abstract

In this study, the synthesis of calcium hexaboride powder via boro/carbothermal reduction (BCTR) using a single-step-processed gel product prepared from commercial boric acid, readily available and low-cost D(-)-Mannitol and calcium carbonate was investigated. The gel product was characterized by means of Fourier Transform Infrared Spectroscopy (FTIR) and Simultaneous Thermal Analysis (STA). The effect of the boro/carbothermal reduction temperature and dwell time on the phase formation were examined with x-ray diffractometry and scanning electron microscopy. CaB6 synthesis was performed with the gel product without additional heat treatment in air to obtain the appropriate C amount in the gel precursor. Ca3B2O6, B4C and Ca2B6O11 were formed as a transitional phase to create CaB6 particles. To understand the formation and consuming mechanism of the transitional phases, thermodynamic calculations were performed based on reactions that probably occurred in the system. The optimum synthesis conditions for the formation of calcium hexaboride were determined as 1400 °C for 12 h in an argon flow.

Download Full Article (PDF)

Keywords

Hexaboride, boro/carbothermal reduction, gel precursor, boric acid, mannitol

References

1 Matkovich, V.I.: Boron and Refractory Borides, Springer Verlag, Berlin, 1977.

2 Tsushinsha, N.: Handbook on High-Melting Point Composites, Ehime, Japan, 1977.

3 Wang, L., Xu, L., Ju, Z., Qian, Y.:A versatile route for the convenient synthesis of rare-earth and alkaline-earth hexaborides at mild temperatures, CrystEngComm., 12, 3923 – 3928, (2010).

4 Siddiqui, N., Koc, R., Mawdsley, J., Carter, D.: Synthesis of submicron/nano sized CaB6 from carbon coated precursors, in Nanostructured Materials and Nanotechnology V, Ceramic Engineering and Science Proceedings, Vol. 32 (eds S. Mathur, S. S. Ray, S. Widjaja and D. Singh), John Wiley & Sons, Inc., 137, 2011.

5 Zheng, S., Min, G., Zou, Z., Yu, H., Han, J.: Synthesis of calcium hexaboride powder via the reaction of calcium carbonate with boron carbide and carbon, J. Am. Ceram. Soc., 84, 2725 – 2727, (2001).

6 Hanagiri, S., Harada, T., Aso, S. et al.: Effects of the addition of metal and CaB6 to magnesia carbon bricks for converters, Taikabutsu Overseas, 13, 20 – 27, (1993).

7 Razavi-Zadeh, H., Mirdamadi, S.T.: Deoxidizing copper with CaB6, JOM, 39, 42 – 47, (1987).

8 Xin, S., Han, X., Liu, S., Liu, Z., Xu, B., Tian, Y., Yu, D.: CaB6 single crystals grown under high pressure and high temperature, J. Cryst. Growth, 313, 47 – 50, (2010).

9 Yildiz, O., Telle, R., Schmalzried, C., Kaiser, A.: Phase transformation of transient B4C to CaB6 during production of CaB6 from colemanite, J. Eur. Ceram. Soc., 25, 3375 – 3381, (2005).

10 Huang, X., Zhong, J., Dou, L., Wang, K.: Combustion synthesis of CaB6 powder from calcium hexaborate and mg, Int. J. Refract. Met. H., 28, 143 – 149, (2010).

11 Angappan, S., Helan, M., Visuvasam, A., Berchmans, L.J., Ananth, V.: Electrolytic preparation of CaB6 by molten salt technique, Ionics, 17, 527 – 533, (2011).

12 Balcı, Ö., Ağaoğulları, D., Duman, İ., Öveçoğlu, M.L.: Synthesis of CaB6 powders via mechanochemical reaction of Ca/B2O3 blends, Powder Technol., 225, 136 – 142, (2012).

13 Shi, L., Gu, Y., Chen, L., Yang, Z., Ma, J., Qian, Y.: Low temperature synthesis and characterization of cubic CaB6 ultrafine powders, Chem. Lett., 32, 958 – 959, (2003).

14 Etourneau, J., Mercurio, J.P. and Hagenmuller, P.: Compounds based on octahedral units: Hexaborides and tetra borides, in: V.I. Matkovitch (ed.), Boron and Refractory Borides, Springer Berlin Heidelberg, New York, 1977.

15 Zhang, L., Min, G., Yu, H., Chen, H., Feng, G.: The size and morphology of fine CaB6 powder synthesized by nanometer CaCO3 as reactant, Key Eng. Mat., 326 – 328, 369 – 372, (2006).

16 Kakiage, M., Shiomi, S., Yanase, I., Kobayashi, H.: Low-temperature synthesis of calcium hexaboride powder via transient boron carbide formation, J. Am. Ceram. Soc., 98, 2724 – 2727, (2015).

17 Kakiage, M., Tominaga, Y., Yanase, I., Kobayashi, H.: Synthesis of boron carbide powder in relation to composition and structural homogeneity of precursor using condensed boric acid-polyol product, Powder Technol., 221, 257 – 263, (2012).

18 Steinberg, H.: Organoboron chemistry, Boron-oxygen and boron-sulfur compounds, (1), John Wiley & Sons Inc., New York, 1964.

19 Silverstein, R.M., Webster, F.X., Kiemle, D.J., Bryce, D.L.: Spectrometric Identification of Organic Compounds, John Wiley & Sons, Inc., 2005.

20 Yanase, I., Ogawara, R., Kobayashi, H.: Synthesis of boron carbide powder from polyvinyl borate precursor, Mater. Lett., 63, 91 – 93, (2009).

21 Najafi, A., Golestani-Fard, F., Rezaie, H.R., Ehsani, N.: Effect of APC addition on precursors properties during synthesis of B4C nano powder by sol-gel process, J. Alloy Compd., 509, 9164 – 9170, (2011).

22 Mondal, S., Banthia, A.K.: Low-temperature synthetic route for boron carbide, J. Am. Ceram. Soc., 25, 287 – 291, (2005).

Copyright

Göller Verlag GmbH

Special and Topcial Issues

Special Issue, 3/2025
Guest Editors:
Olaf Krause and Christian Dannert
Advances in Refractories

Topical Issue, 3/2017
Guest Editors:
Waltraud M. Kriven and Gregor J. G. Gluth
Geopolymers

Special Issue, 1/2017
Guest Editor:
Alexander Michaelis
6th International Congress on Ceramics (ICC6)

Topical Issue, 2/2016
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advan-ced steel technologies; A challenge for refractory materials and systems.

Topcial Issue, 4/2015
Low Temperature Co-fired Ceramics - LTCC

Topcial Issue, 2/2015
Status of Additive Manufacturing with Ceramics

Topical Focus, 4/2014
Materials Processing Science with Lasers as Energy Sources

Topical Issue, 2/2014
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advanced steel technologies; A challenge for refractory materials and systems.

Special Issue, 2/2013
Guest Editor:
Alexander Michaelis
Ceramic Materials and Components for Energy and Environmental Applications

Topical Issue, 1/2013
Ceramic Processing Science with Lasers as Energy Sources

Printed version

jcst 2015 02 cover

Order journal subscription
 

© 2009-2025 Göller Verlag GmbH