Synthesis and Dielectric Properties of Thin-Layered (La,Nd)TiO2N Perovskites
J. Ahchawarattaworn1, D.P. Thompson1, F. Azough2, R. Freer2
1 School of Chemical Engineering and Advanced Materials, University of Newcastle, Newcastle upon Tyne, NE1 7RU, U.K.
2 School of Materials, University of Manchester, Manchester M13 9PL, U.K.
received June 3, 2015, received in revised form August 28, 2015, accepted October 5, 2015
Vol. 7, No. 1, Pages 39-46 DOI: 10.4416/JCST2015-00022
Abstract
Dielectric measurements made on thin layers of oxynitride of composition (La,Nd)TiO2N deposited on substrates of the equivalent pure oxides gave high and variables values for the relative permittivity, and very high values of dielectric loss, showing that the samples were significantly conducting. This is believed to be due to reduction taking place during the nitridation step, the use of ammonia (by far the most convenient and effective nitriding agent for this purpose) resulting in the simultaneous production of active atomic hydrogen which easily diffuses through both the surface oxide and the simultaneously forming layer of oxynitride to give compositions of the type (La,Nd)2TiIV2-xTiIIIxO7-x/2 and LaxNd1-xTi4+1-yTi3+yO2-y/2N respectively. It is well established that the presence of Ti3+ in titanium oxides and oxynitrides readily promotes conductivity. These results explain the diverse dielectric property measurements reported by previous researchers working on oxynitride materials, and show that alternative nitridation methods are needed in order to determine correct values of dielectric properties of pure oxynitride materials.
Download Full Article (PDF)
Keywords
Oxynitrides, perovskites, XRD characterisation, dielectric properties.
References
1 Thompson, D.P.: Oxynitride research in the nano era, Mater. Sci. Forum, 554, 1 – 10, (2007).
2 Marchand, R., Pors, F., Laurent, Y.: Preparation and characterisation of new oxynitrides with a perovskite structure, (in French), Rev. Int. Hautes Tempér. Réfract. Fr., 23, 11 – 15, (1986).
3 Gouin, X., Marchand, R., Laurent, Y., Gervais, F.: Infrared dielectric response of BaTaO2N, Sol. State Commun., 93, 857 – 9, (1995).
4 Kim, Y.-I., Woodward, P.M., Baba-Kishi, K.Z., Tai, C.W.: Characterization of the structural, optical and dielectric properties of oxynitride perovskites AMO2N (A = Ba,Sr,Ca; M=Ta,Nb), Chem. Mater., 16, 1267 – 76, (2004).
5 Marchand, R., Laurent, Y., Guyader, J., L'Haridon, P., Verdier, P.: Nitrides and oxynitrides: preparation, crystal chemistry and properties, J. Eur. Ceram. Soc., 8, 197 – 213, (1991).
6 Clarke, S.J., Guinot, B.P., Michie, C.W., Calmont, M.J.C., Rosseinsky, M.J.: Oxynitride perovskites: synthesis and structures of LaZrO2N, NdTiO2N and LaTiO2N and comparison with oxide perovskites, Chem. Mater., 14, 288 – 94, (2002).
7 Ziani, A., Le Pavin-Thivet, C., Le Gendre, L., Fasquelle, D., Carru, J.C., Tessier, F., Pinel J.: Structural and dielectric properties of oxynitride perovskite LaTiOxNy thin films, Thin Solid Films, 517, 544 – 49, (2008).
8 Ebbinghaus, S.G., Abicht, H.P., Dronskowski, R., Moeller, T., Reller, A. Weidenkaff, A.: Perovskite-related oxynitrides – recent developments in synthesis, characterization and investigations of physical properties, Prog. Sol. State Chem., 37, 173 – 205, (2009).
9 Masubuchi, Y., Sun, S.-K., Kikkawa, S.: Processing of dielectric oxynitride perovskites for powders, ceramics, compacts and thin films, Dalton T., 44, 10570 – 81, (2015).
10 Wang, S.F., Hsu, Y.F., Wang, Y.R., Cheng, L.T., Hsu, Y.C., Chu, J.P., Huang, C.Y.: Densification, microstructural evolution and dielectric properties of Ba6 – 3x(Sm1-yNdy)8+2xTi18O54 microwave ceramics, J. Eur. Ceram. Soc., 26, 1629 – 35, (2006).
11 Paul, A.F., Robert, E.N.: La2Ti2O7 ceramics, J. Am. Ceram. Soc., 74, 2876 – 81, (1991).
12 Takahashi, J., Kageyama, K., Kodaira, K.: Microwave dielectric properties of lanthanide titanate ceramics, Jap. J. Appl. Phys. 1, 32, 4327 – 31.
13 Shao, Z., Saitzek, S., Roussel, P., Mentré, O., Prihor-Gheorghiu, F., Mitoseriu, L., Desfeux, R.: Structural and dielectric/ferroelectric properties of (La1-xNdx)2Ti2O7 synthesized by sol-gel route., J. Solid State Chem., 183, 1652 – 62, (2010).
14 Ioroi, T., Senoh, H., Yamazaki, S., Siroma, Z., Fujiwara, N., Yasuda, K.: Stability of corrosion-resistant Magnéli-phase Ti4O7-supported PEMFC catalysts at high potentials, J. Electrochem. Soc., 155, B321 – 6, (2008).
15 Egerton, T.A., Kessell, L.M., Tooley, I.R., Wang, L.: Photogreying of TiO2 nanoparticles, J. Nanopart. Res., 9, 251 – 60, (2007).
16 Ebbinghaus, S.G., Aguiar, R. Weidenkaff, A., Gsell, S., Reller, A.: Topotactical growth of thick perovskite oxynitride layers by nitridation of single crystalline oxides. Solid State Sci., 10, 709 – 16, (2008).
17 Akishige, Y., Kobayashi, M., Ohi, E., Sawaguchi, E.: Dielectric and ferroelectric properties in the low-temperature phase of strontium niobate, J. Phys. Soc. Jap., 55, 2270 – 7, (1986).
18 Bobnar, V., Lunkenheimer, P., Hemberger, J., Loidl, A., Lichtenberg, F., Mannhart, J.: Dielectric properties and charge transport in the (Sr,La)NbO3.5-x system, Phys. Rev. B., 65, 155115, (2002).
19 Sun, S.-K., Zhang, Y.-R., Masubuchi, Y., Motohashi, T. Kikkawa, S.: Additive sintering, post-annealing and dielectric properties of SrTaO2N, J. Am. Ceram. Soc., 97, 1023 – 7, (2014).
20 Kim, Y.-I.: Effects of KCl flux on the morphology, anion composition and chromaticity of perovskite oxynitrides, CaTaO2N, SrTaO2N and LaTaON2, Ceram. Int., 40, 5275 – 81, (2014).
21 Motohashi, T., Hamade, Y., Masubuchi, Y., Takeda, T., Murai, K., Yoshiasa, K., Kikkawa, S.: Structural phase transitions in the perovskite-type tantalum oxynitrides Ca1-xEuxTa(O,N)3, Mater. Res. Bull., 44, 1899 – 1905, (2009).
22 Sun, S.-K., Motohashi, T., Masubuchi, Y., Kikkawa, S.: Direct synthesis of SrTaO2N from SrCO3/Ta3N5 involving CO evolution, J. Eur. Ceram. Soc., 34, 4451 – 55, (2014).
Copyright
Göller Verlag GmbH