Articles
All articles | Recent articles
Small-Size Low-Loss Bandpass Filters on Substrate-Integrated Waveguide Capacitively Loaded Cavities Embedded in Low Temperature Co-Fired Ceramics
V. Turgaliev1, D. Kholodnyak1, J. Müller2, and M.A. Hein2
1 St Petersburg Electrotechnical University "LETI", 5 Prof. Popov Str., 197376 St Petersburg, Russia
2 Ilmenau University of Technology, 98693 Ilmenau, Germany
received September 1, 2015, received in revised form October 26, 2015, accepted November 13, 2015
Vol. 6, No. 4, Pages 305-314 DOI: 10.4416/JCST2015-00053
Abstract
The design of microwave filters for portable electronics is complicated by conflicting requirements that must be met simultaneously such as high selectivity, low insertion loss and compact size. Substrate-integrated waveguide (SIW) technology allows the design of low-profile high-Q resonators and low-loss filters based on this. However, SIW filters are not well suited for telecommunication applications because of their remarkably large size in plane. The size of a SIW cavity can be dramatically reduced with the use of capacitive loading. Capacitively loaded cavities (CLCs) operating in the TM110 mode are shown to be as small as 1/8 of the guided wavelength and even smaller, i.e. comparable in size with lumped-element resonators. Although the unloaded Q-factor decreases proportionally to cavity size, miniaturized CLCs can exhibit a much higher Q-factor than that of lumped-element resonators. This paves the way for designing small-size and low-loss filters for wireless communications and different applications. Miniaturized capacitively loaded SIW cavities are favorably implemented by means of low-temperature co-fired ceramics (LTCC) technology. The goal of the paper is to demonstrate the manifold possibilities and flexibility offered by LTCC technology for the design of advanced microwave filters on CLCs. Different design and manufacturing aspects are considered. Various design examples of high-performance LTCC resonators and filters for single- and dual-band wireless applications are presented. The designed resonators and filters were manufactured using the commercial DuPont Green Tape 951 LTCC system. The LTCC filters on miniaturized CLCs are shown to be advantageous with regard to small size, low loss, and absence of spurious response over a wide frequency range.
Download Full Article (PDF)
Keywords
Substrate-integrated waveguide (SIW), low temperature co-fired ceramics (LTCC), capacitively loaded cavities, dual-mode resonators, bandpass filters.
References
1 Bozzi, M., Georgiadis, M.A., Wu, K.: Review of substrate-integrated waveguide circuits and antennas, IET Microw. Antenna P., 5, [8], 909 – 920, (2011).
2 Lee, J.-H., Pinel, S., Papapolymerou, J., Laskar, J., Tentzeris, M.M.: Low loss LTCC cavity filters using system-on-package technology at 60 GHz, IEEE T. Microw. Theory, 53, [12], 3817 – 3824, (2005).
3 Potelon, B., Bohorquez, J.-C., Favennec, J.-F., Quendo, C., Rius, E., Person, C.: Design of Ku-band filter based on substrate-integrated circular cavities (SICCs). In: 2006 IEEE MTT-S Int. Microw. Symp. Dig. San Francisco, California, 1237 – 1240, (2006).
4 Shen, T.-M., Chen, C.-F., Huang, T.-Y., Wu, R.-B.: Design of vertically stacked waveguide filters in LTCC, IEEE T. Microw. Theory, 55, [8], 1771 – 1779, (2007).
5 Zhang, X.-C., Yu, Z.-Y., Xu, J.: Novel band-pass substrate integrated waveguide (SIW) filter based on complementary split ring resonators (CSRRS), Prog. Electromagn. Res., 72, 39 – 46, (2007).
6 Potelon, B., Favennec, J.-F., Quendo, C., Rius, E., Person, C., Bohorquez, J.-C.: Design of a substrate integrated waveguide (SIW) filter using a novel topology of coupling, IEEE Microw. Wirel. Co., 18, [9], 596 – 598, (2008).
7 Tsai, W.-L., Wu, R.-B.: Tri-band filter design using substrate integrated waveguide resonators in LTCC. In: 2010 IEEE MTT-S Int. Microw. Symp. Dig. Anaheim, California, 445 – 448, (2010).
8 Xu, Z.Q., Shi, Y., Wang, P., Liao, J.X., Wei, X.B.: Substrate integrated waveguide (SIW) filter with hexagonal resonator, J. Electromagnet. Wave, 26, [11 – 12], 1521 – 1527, (2012).
9 Xu, L.-J., Wang, J.P., Guo, Y.-X., Wu, W.: Double-folded substrate integrated waveguide band-pass filter with transmission zeros in LTCC, J. Electromagnet Wave., 27, [1], 96 – 103, (2013).
10 Gong, X., Margomenos, A., Liu, B., Chappell, W.J., Katehi, L.P.B.: High-Q evanescent-mode filters using silicon micromachining and polymer stereolithography (SL) processing. In: 2004 IEEE MTT-S Int. Microw. Symp. Dig. Fort Worth, Texas, 433 – 436, (2004).
11 Ferrand, P., Baillargeat, D., Verdeyme, S., Puech, J., Lahti, M., Jaakola, T.: LTCC reduced-size bandpass filters based on capacitively loaded cavities for Q-band application, In: 2005 IEEE MTT-S Int. Microw. Symp. Dig. Long Beach, California, 1789 – 1792, (2005).
12 Rigaudeau, L., Ferrand, P., Baillargeat, D., Bila, S., Verdeyme, S., Lahti, M., Jaakola, T.: LTCC 3-D resonators applied to the design of very compact filters for Q-band applications, IEEE T. Microw. Theory, 54, [6], 2620 – 2627, (2006).
13 Joshi, H., Sigmarsson, H.H., Peroulis, D., Chappell, W.J.: Highly loaded evanescent cavities for widely tunable high-Q filters. In: 2007 IEEE MTT-S Int. Microw. Symp. Dig. Honolulu, Hawaii, 2133 – 2136, (2007).
14 Kushta, T., Harada, T.: New 3-D design of filtering components using multilayer board technologies. In: Proc. 38th Eur. Microw. Conf., Amsterdam, the Netherlands, 218 – 221, (2008).
15 Turgaliev, V., Kholodnyak, D., Vendik, I., Stöpel, D., Humbla, S., Müller, J., Hein, M.A.: LTCC highly loaded cavities for the design of single- and dual-band low-loss miniature filters. In: Proc. 40th Eur. Microw. Conf., Paris, France, pp. 180 – 183, (2010).
16 Turgaliev, V., Kholodnyak D., Vendik, I.: Small-size dual-band filters on capacitively loaded cavities. In: Proc. 43rd Eur. Microw. Conf., Nuremberg, Germany, 660 – 663, (2013).
17 Kholodnyak, D.V., Turalchuk, P.A., Zameshaeva, E. Yu.: Dual-frequency immittance inverter with a stop-band between the operation frequencies based on one-dimensional metamaterials. Patent RU 2463690 C2, (2012), (in Russian).
18 Kholodnyak, D., Turgaliev, V., Vorobev, E.: Advanced microwave filters in LTCC and PCB technologies. In: Proc. 2014 Asia-Pacific Microw. Conf., Sendai, Japan, 88 – 90, (2014).
19 Kholodnyak, D., Turgaliev, V., Zameshaeva, E.: Dual-band immittance inverters on dual-composite right/left-handed transmission line (D-CRLH TL). In: Proc. 9th German Microw. Conf., Nuremberg, Germany, 60 – 63, (2015).
Copyright