Slurry-Based Powder Beds for the Selective Laser Sintering of Silicate Ceramics
T. Mühler1, C. Gomes2, M.E. Ascheri2, D. Nicolaides2, J.G. Heinrich1, J. Günster1,2
1 Institute of Non-Metallic Materials, Clausthal University of Technology, Zehntnerstrasse 2a, D-38678 Clausthal-Zellerfeld, Germany
2 BAM Federal Institute of Materials Research and Testing, Unter den Eichen 87, D-12205 Berlin, Germany
received February 6, 2015, received in revised form April 10, 2015, accepted April 24, 2015
Vol. 6, No. 2, Pages 113-118 DOI: 10.4416/JCST2015-00007
Abstract
Selective laser sintering of ceramic powders is a promising technique for the additive manufacturing of complex- and delicate-shaped ceramic parts. Most techniques have in common that the powder to be sintered is spread to a thin layer as a dry powder by means of a roller or shaker system. These layers have a relatively low density. On the other hand, appreciable densities can be reached with the use of ceramic slurries as the starting material. Therefore, the layer-wise slurry deposition (LSD) process has been developed. Layer stacks, i.e. powder beds, built up by employing the LSD technology exhibit a density comparable to ceramic powder compacts processed by means of conventional forming technologies. Writing the layer information with a focused laser beam in these dense ceramic powder compacts enables the manufacture of ceramic bodies with a high density and precision in contour.
Download Full Article (PDF)
Keywords
LSD, powder bed, SLS, additive manufacturing, silicate ceramics
References
1 ASTM F2792 – 10 Standard Terminology for Additve Manufacturing Technologies, ASTM, USA, (2012).
2 Travitzky, N., Bonet, A., Dermeik, B., Fey, T., Filbert-Demut, I., Schlier, L., Schlordt, T., Greil, P.: Additive manufacturing of ceramic-based materials, Adv. Eng. Mater., 16, [6], 729 – 754, (2014).
3 Deckers, J., Vleugels, J., Kruth, J.-P.: Additive manufacturing of ceramics: A review, J. Ceram. Sci. Tech., 5, [4], 245 – 260, (2014).
4 Mcguffin-Cawley, J.D.: Manufacturing technology: Rapid prototyping, 415 – 437 in Ceram. Sci. Technol. Edited by R. Riedel and I.-W. Chen. Wiley-VCH Verlag GmbH & Co. KGaA, 2011.
5 Sigmund, W.M., Bell, N.S., Bergström, L.: Novel powder-processing methods for advanced ceramics, J. Am. Ceram. Soc., 83, [7], 1557 – 1574, (2000).
6 Günster, J., Engler, S., Heinrich, J.G.: Forming of complex shaped ceramic products via layer-wise slurry deposition (LSD), Bull. Eur. Ceram. Soc., 1, 25 – 28, (2003).
7 Tian, X., Günster, J., Melcher, J., Li, D., Heinrich, J.G.: Process parameters analysis of direct laser sintering and post treatment of porcelain components using Taguchi's method, J. Eur. Ceram. Soc., 29, 1903 – 15, (2009).
8 Muehler, T., Heinrich, J., Gomes, C.M., Günster, J.: Slurry-based additive manufacturing of ceramics, Int. J. Appl. Ceram. Technol., 12, [1], 18 – 25, (2015).
9 Yen, H.-C.: Experimental studying on development of slurry-layer casting system for additive manufacturing of ceramics, Int. J. Adv. Manuf. Technol., DOI 10.1007/s00170 – 014 – 6534 – 8
10 Tang, H.-H., Yen, H.-C.: Slurry-based additive manufacturing of ceramic parts by selective laser burn-out, J. Eur. Ceram. Soc., 35, 981 – 987, (2015).
11 Huson, D., Hoskins, S.: 3D printed ceramics for tableware, Artists/Designers and specialist applications, Key Eng. Mat., 608, 351 – 357, (2014).
12 Juste, E., Petit, F., Lardot, V., Cambier, F.: Shaping of ceramic parts by selective laser melting of powder bed, J. Mater. Res., 29, [17], 2086 – 2094, (2014).
Copyright
Göller Verlag GmbH