• Home
  • Contact
  • Login
  • Privacy
  • Imprint

Search

Journal of Ceramic Science and Technology

The Journal of Ceramic Science and Technology publishes original scientific articles on all topics of ceramic science and technology from all ceramic branches. The focus is on the scientific exploration of  the relationships between processing, microstructure and properties of sintered ceramic materials as well as on new processing routes for innovative ceramic materials. The papers may have either theoretical or experimental background. A high quality of publications will be guaranteed by a thorough double blind peer review process.

The Journal is published by Göller Verlag GmbH on behalf of the Deutsche Keramische Gesellschaft (DKG). Edited by Yu-Ping Zeng, Shanghai Institute of Ceramics, Chinese Academy of Sciences, China.

  • Home
  • Early view
  • Articles
    • All articles
    • Recent Articles
    • Early Views
  • Issues
  • Submit an article
  • Guidelines for Referees
  • Guidelines for Authors
  • Open Access
  • Editorial Board
  • Copyright
  • Contact
  • Order journal / article
  • Customer area
  • Terms of Service

Journal Metrics

Web of science
Impact Factor: 1,220
Impact Factor without Journal Self Cites: 1,060
5 Year Impact Factor: 0,818

Scopus
Scimago Journal Rank (SJR):  0,378

 

Prices

Authors
1,300 € Open Access

Print Subscription
62 € per year

view all subscriptions

 

Payment methods

 Credit card

 Invoice

 Wire transfer

 

Articles

All articles  |  Recent articles

Fabrication of MAX-Phase-Based Ceramics by Three-Dimensional Printing

Y. Ma1, X. Yin1, X. Fan1, N. Travitzky2, P. Greil2

1 Science and Technology on Thermostructural Composite Materials Laboratory, Northwestern Polytechnical University, Xi¡¯an, Shaanxi, 710072, PR China
2 Department of Materials Science (Glass and Ceramics), University of Erlangen-Nuremberg, Erlangen, Germany.

received February 3, 2015, received in revised form March 1, 2015, accepted April 1, 2015

Vol. 6, No. 2, Pages 87-94   DOI: 10.4416/JCST2015-00006

Abstract

Three-dimensional printing (3DP) is a flexible and cost-effective method for direct digital manufacturing that provides capabilities for creating a wide range of part geometries in a broad variety of materials. Recently, a combined process of 3DP and reactive melt infiltration (RMI) has been applied to fabricate MAX-phase-based ceramics, exhibiting great potential in the fabrication of bulk compounds with complicated shape. This paper briefly summarizes the fabrication of Ti3AlC2- and Ti3SiC2-based ceramics with the combined process. 3DP facilitates the prior design of a porous preform with specific pore distribution and microstructure, which is beneficial to the control of the volume change of the following reaction in the RMI process, promoting the near-net-shape fabrication of MAX-phase-based ceramics with high flexibility in component geometry.

Download Full Article (PDF)

Keywords

Three-dimensional printing, RMI, Ti3SiC2, Ti3AlC2.

References

1 Barsoum, M.W., Radovic, M.: Mechanical properties of the MAX phases in encyclopedia of materials science and technology, Elsevier, Amsterdam, (2004).

2 Barsoum, M.W., El-Raghy, T.: Synthesis and characterization of a remarkable ceramic: Ti3SiC2, J. Am. Ceram. Soc., 79, 1953 – 1956, (1996).

3 Zhou, Y., Sun, Z., Chen, S., Zhang, Y.: In-situ hot-pressing solid-liquid reaction synthesis of dense titanium silicon carbide bulk ceramics, Mater. Res. Innov., 2, 142 – 146, (1998).

4 Barsoum, M.W.: The MN+1AXN Phases: A new class of Solids; thermodynamically stable nano laminates, Prog. Solid State Ch., 28, 201 – 281, (2000).

5 Radhakrishnan, R., Henager, C.H., Brimball, J.L., Bhaduri, S.B.: Synthesis of Ti3SiC2/SiC and TiSi2/SiC composites using displacement reactions in the Ti–Si–C system, Scripta. Mater., 34, 1809 – 1814, (1996).

6 Fan, X., Yin, X., He. S., Zhang, L., Cheng, A.: Friction and wear behaviors of C/C-SiC composites containing Ti3SiC2, Wear, 27, 274 – 275, (2012).

7 Zhang, H., Wang, X., Nickel, K.G., Zhou, Y.: Experimental and thermodynamic study of the hydrothermal oxidation behavior of Ti3SiC2 powders, Scripta. Mater., 59, 746 – 749, (2008).

8 Yin, X., He, S., Zhang, L., Fan, A., Cheng, L., Tian, G., Li, T.: Fabrication and characterization of a carbon fiber reinforced carbon-silicon carbide-titanium silicon carbide hybrid matrix composite, Mater. Sci. Eng. A, 527, 835 – 841, (2010).

9 Fan, X., Yin, X.: Microstructure and properties of carbon fiber reinforced SiC matrix composites containing Ti3SiC2, Adv. Eng. Mater., 16, 670 – 683, (2014).

10 Yin, X., Travitzky, N., Greil, P.: Reactive infiltration processing of Ti3AlC2 and Ti3SiC2-based composites, Nova Science Publishers, New York Inc. (2012).

11 Goto, T., Hirai, T.: Chemically vapor deposited Ti3SiC2, Mater. Res. Bull., 22, 1195 – 1202, (1987).

12 Jacques, S., Fakih, H., Viala, J.C.: Reactive chemical vapor deposition of Ti3SiC2 with and without pressure pulses: effect on the ternary carbide texture, Thin Solid Films, 518, 5071 – 5077, (2010)

13 3 Yang, C., Jin, S.Z., Liang, B.Y., Jia, S.S.: Low-temperature synthesis of high-purity Ti3AlC2 by MA-SPS technique, J. Eur. Ceram. Soc., 29, 181 – 185, (2009).

14 Li, S., Zhai, H.: Synthesis and reaction mechanism of Ti3SiC2 by mechanical alloying of elemental Ti, Si, and C powders, J. Am. Ceram. Soc., 88, 2092 – 2098, (2005).

15 Gauthier, V., Cochepin, B., Dubois, S.: Self-propagating high-temperature synthesis of Ti3SiC2: Study of the reaction mechanisms by time-resolved X-ray diffraction and infrared thermography, J. Am. Ceram. Soc., 89, 2899 – 2907, (2006).

16 Meng, F., Liang, B., Wang, M.: Investigation of formation mechanism of Ti3SiC2 by self-propagating high-temperature synthesis, Int. J. Refract. Met. H. 41, 152 – 161, (2013).

17 Yeh, C.L., Shen, Y.G.: Effects of using Al4C3 as a reactant on formation of Ti3AlC2 by combustion synthesis in SHS mode, J. Alloy. Compd., 473, 408 – 413, (2009).

18 Li, S., Song, G., Zhou, Y.: Dense and fine-grained SiC/Ti3Si(Al)C2 composite and its high-temperature oxidation behavior, J. Eur. Ceram. Soc., 32, 3435 – 3444, (2012).

19 Tzenov, N.V., Barsoum, M.W.: Synthesis and characterization of Ti3AlC2, J. Am. Ceram. Soc., 83, 825 – 832, (2000)

20 Han, J.H., Hwang, S.S., Lee, D., Park S.W.: Synthesis and mechanical properties of Ti3AlC2 by hot pressing TiCx/Al powder mixture, J. Eur. Ceram. Soc., 28, 979 – 988, (2008).

21 Gao, N.F., Li, J.T., Zhang, D.: Rapid synthesis of dense Ti3SiC2 by spark plasma sintering, J. Eur. Ceram. Soc., 22, 2365 – 2370, (2002).

22 Zhou, Y., Zhang, H., Liu, M.: Preparation of TiC free Ti3SiC2 with improved oxidation resistance by substitution of si with al, Mater. Res. Innov., 8, 97 – 102, (2004).

23 Arunajatesan, S., Carim, A.H.: Synthesis of titanium silicon carbide, J. Am. Ceram. Soc., 78, 667 – 672, (1995).

24 Sun, W., Dcosta, D., Lin, F., El-Raghy, T.: Freeform fabrication of Ti3SiC2 Powder-based structures part I-integrated fabrication process, J. Mater. Proc. Technol., 127, 343 – 351, (2002).

25 Sachs, E., Cima, M., Williams, D., Brancazio, D., Cornie, J.: Three dimensional printing rapid tooling and prototypes directly from a CAD model, CIRP Ann. Manuf. Techn., 39, 201 – 204, (1990).

26 Sachs, E., Cima, M., Williams, D., Brancazio, D., Cornie, J.: Three dimensional printing rapid tooling and prototypes directly from a CAD model, J. Manuf. Sci. Eng., 114, 481 – 488, (1992).

27 Chua, C.K., Leong, K.F., Lim, C.S.: Rapid prototyping: principles and applications, 3rd edition. World Scientific, Singapore, 2010.

28 Song, J.H., Edirisinghe, M.J., Evans, J.R.G.: Formulation and multilayer jet printing of ceramic inks, J. Am. Ceram. Soc., 82, 3374 – 3380, (1999).

29 Sachs, E., Cima, M., Bredt, J., Curodeau, A., Fan, T., Brancazio, D.: CAD-casting: Direct fabrication of ceramic shells and cores by three-dimensional printing, Manuf. Rev., 5, 117 – 126, (1992).

30 Lejeune, M., Chartier, T., Dossou-Yovo, C., Noguera, R., Ink-jet printing of ceramic micro-pillar arrays, J. Eur. Ceram. Soc., 29, 905 – 911, (2009).

31 Greil, P.: Biomorphous ceramics from lignocellulosics, J. Eur. Ceram. Soc., 21, 105 – 118, (2001).

32 Greil, P.: Near net shape manufacturing of ceramic, Mater. Chem. Phys., 61, 64 – 68, (1999).

33 Windsheimer, H., Travitzky, N., Hofenauer, A., Greil, P.: Laminated object manufacturing of preceramic-paper-derived SiSiC composites, Adv. Mater., 19, 4515 – 4519, (2007).

34 Moon, J., Caballero, A.C.: Fabrication of functionally graded reaction infiltrated SiC-si composite by three-dimensional printing (3DP) process, Mater. Sci. Eng. A, 298, 110 – 119, (2001).

35 Travitzky, N., Zimmermann, K., Melcher, R., Greil, P.: From polysaccharides to SiSiC composites by 3D printing, Ceram. Trans., 175, 37 – 45, (2006).

36 Fu, Z., Schlier, L., Travitzky, N., Greil, P.: Three-dimensional printing of SiSiC lattice truss structures, Mater. Sci. Eng. A,, 560, 851 – 856, (2013).

37 Yin, X., Travitzky, N., Greil, P.: Near-net-shape fabrication of Ti3AlC2-based composites, Int. J. Appl. Ceram. Technol., 4, 184 – 190, (2007).

38 Yin, X., Travitzky, N., Greil, P.: Three-dimensional printing of nanolaminated Ti3AlC2 toughened TiAl3–Al2O3 composites, J. Am. Ceram. Soc., 90, 2128 – 2134, (2007).

39 Nan, B., Yin, X., Zhang, L., Cheng, L.: Three-dimensional printing of Ti3SiC2-based ceramics, J. Am. Ceram. Soc., 94, 969 – 972, (2011).

40 Ma, Y., Yin, X., Fan, X., Wang, L., Greil, P., Travizky. N.: Near-Net-shape fabrication of Ti3SiC2-based ceramics by three-dimensional printing, Int. J. Appl. Ceram. Technol., 12, 71 – 80, (2015).

41 Voytovych, R., Bougiouri, V., Calderon, N.R., Narciso, J., Eustathopoulos, N.: Reactive infiltration of porous graphite by NiSi alloys, Acta Mater., 56, 2237 – 2246, (2008).

42 Fan, X., Yin, X., Wang, L., Zhang, L., Cheng, L.: Processing, microstructure and ablation behavior of C/SiC-Ti3SiC2 composites fabricated by liquid silicon infiltration, Corros. Sci., 74, 98 – 05, (2013).

43 Wan, D., Zhou, Y., Hu, C., Bao, Y.: Improved strength-impairing contact damage resistance of Ti3Si(Al)C2/SiC composites, J. Eur. Ceram. Soc., 27, 2069 – 2076, (2007).

44 Lu, C., Yin, X., Li, X.: A Novel in-situ synthesis route of Ti3SiC2-SiC Composite by Liquid Silicon Infiltration, J. Inorg. Mater., 25, 1003 – 1008, (2010).

45 Shan, D., Yan, G., Zhou, L., Li, C., Li, J., Liu, G., Feng, J.: Synthesis of Ti3SiC2 bulks by infiltration method, J. Alloy. Compd., 509, 3602 – 3605, (2011).

46 Hwang, S., Han, J., Lee, D., Park, S.: Synthesis of Ti3SiC2 by infiltration of molten si, J. Alloy. Compd., 509, 336 – 339, (2011).

47 Kang, Y., Fey, T., Greil, P.: Synthesis of Ti2SnC MAX phase by mechanical activation and melt infiltration, Adv. Eng. Mater., 14, 85 – 91, (2012).

48 Lenz, F., Krenkel, W.: Carbon fiber reinforced ceramics based on reactive melt infiltration processes, J. Korean Ceram. Soc., 49, 287 – 294, (2012).

49 Messner, R.P., Chiang, Y.M.: Liquid-phase reaction-bonding of silicon carbide using alloyed silicon–molybdenum melts, J. Am. Ceram. Soc., 73, 1193 – 1200, (1990).

50 Travitzky, N., Bonet, A., Dermeik, B., Fey, T., Filber-Demut, I., Schlier, L., Schlordt, T., Greil, P.: Additive manufacturing of ceramic-based materials, Adv. Eng. Mater., 16, 729 – 754, (2014).

51 Leukers, B., Gulkan, H., Irsen, S.H., Milz, S., Tille, C., Schieker, M.: Hydroxyapatite scaffolds for bone tissue engineering made by 3D printing, J. Mater. Sci. Mater. Med., 16, 1121 – 1124, (2005).

52 Utela, B., Storti, D., Anderson, R., Ganter, M.: A review of process development steps for new material systems in three dimensional printing (3DP), J. Manuf. Process., 10, 96 – 104, (2008).

53 Sachs, E.M., Cima, M.J., Caradonna, M.A.: Jetting layers of powder and the formation of fine powder beds thereby, U.S. Patent and Trademark Office, Massachusetts Institute of Technology, 6, 596, 224, (2003).

54 Fierz, F.C., Beckmann, F., Huser, M., Irsen, S.H., Leukers, B., Witte, F., Degistirici, Ö., Andronache, A., Thie, M., Müller, B.: The morphology of anisotropic 3D-printed hydroxyapatite scaffolds, Biomaterials, 29, 3799 – 3806, (2008).

55 Butscher, A., Bohner, M., Roth, C. Ernstberger, A., Heuberger, C., Doebelin, N., Rohr, P.R.V., Müller, R.: Printability of calcium phosphate powders for three-dimensional printing of tissue engineering scaffolds, Acta Biomater., 8, 373 – 385, (2012).

56 Fan, X., Yin, X., Wang, L., Greil, P., Travitzky, N.: Synthesis of Ti3SiC2-based materials by reactive melt infiltration, Int. J. Refract. Met. H., 45, 1 – 7, (2014).

57 Wagner, F., Garcia, D.E., Krupp, A., Claussen, N.: Interpenetrating Al2O3-TiAl3 alloys produced by reactive infiltration, J. Eur. Ceram. Soc., 19, 2449 – 2453, (1999).

58 Chen, J., Li, J., Zhou, Y.: In-situ synthesis of Ti3AlC2/TiC-Al2O3 composites from TiO2-Al-C system, J. Mater. Sci. Tech., 22, 455 – 458, (2006).

59 Yu, R., Zhan, Q., He, L., Zhou, Y., Ye, H.: Si-induced twinning of TiC and formation of Ti3SiC2 platelets, Acta. Mater., 50, 4127 – 4135, (2002).

60 Lina, Z., Zhuo, M., Zhou, Y., Li, M., Wang, J.: Microstructural relationships between compounds in the ti-si-C system, Scripta Mater., 55, 445 – 448, (2006).

61 Wang, L., Yin, X., Fan, X., Greil, P., Travitzky, N.: Ti3Si(Al)C2-based ceramics fabricated by reactive melt infiltration with Al70Si30 alloy, J. Eur. Ceram. Soc., 34, 1493 – 1499, (2014).

62 Yu, R., He, L., Ye, H., Effects of Si and Al on twin boundary energy of TiC, Acta Mater., 51, 2477 – 2484, (2003).

Copyright

Göller Verlag GmbH

Special and Topcial Issues

Topical Issue, 3/2017
Guest Editors:
Waltraud M. Kriven and Gregor J. G. Gluth
Geopolymers

Special Issue, 1/2017
Guest Editor:
Alexander Michaelis
6th International Congress on Ceramics (ICC6)

Topical Issue, 2/2016
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advan-ced steel technologies; A challenge for refractory materials and systems.

Topcial Issue, 4/2015
Low Temperature Co-fired Ceramics - LTCC

Topcial Issue, 2/2015
Status of Additive Manufacturing with Ceramics

Topical Focus, 4/2014
Materials Processing Science with Lasers as Energy Sources

Topical Issue, 2/2014
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advanced steel technologies; A challenge for refractory materials and systems.

Special Issue, 2/2013
Guest Editor:
Alexander Michaelis
Ceramic Materials and Components for Energy and Environmental Applications

Topical Issue, 1/2013
Ceramic Processing Science with Lasers as Energy Sources

Printed version

jcst 2015 02 cover

Order journal subscription
 