Manufacture of Rotationally Symmetric Multilayer Refractory Devices for Steel Casting Applications by Spiral Winding of Ceramic Green Tapes
D. Jakobsen1, R. Hammerbacher1, S. Dudczig2, T. Fey1, A. Roosen1
1 University of Erlangen-Nuremberg, Department of Materials Science, Glass and Ceramics, D-91058 Erlangen, Germany
2 Technische Universität Bergakademie Freiberg, Institute of Ceramics, Glass and Construction Materials, D-09599 Freiberg, Germany
received Nov 11, 2013, received in revised form Jan 22, 2014, accepted Mar 21, 2014
Vol. 5, No. 2, Pages 137-144 DOI: 10.4416/JCST2013-00040
Abstract
In order to create rotationally symmetric refractory devices from ceramic green tapes, the spiral winding method, which is mainly known from the paper industry, was applied. Different green tapes with varying properties with regard to shrinkage, porosity and Young's modulus were used to generate multilayer tubes with the spiral winding and the cold low pressure lamination technique. The tubes were fired in air and their microstructure was investigated. Thermal shock tests were conducted to evaluate the applicability of the fabricated structures for refractory applications. The correlation between the microstructure and thermal shock behaviour of the tubes is discussed.
Download Full Article (PDF)
Keywords
Keywords: Spiral winding, green tapes, refractories, thermal shock
References
1 Buhr, A.: Refractories for steel secondary metallurgy, CN-Refractories, 6, [3], 19 – 30, (1999).
2 Aneziris, C.G., Jin, S.L., Li, Y.W., Roungos, V.: Interactions of carbon nanotubes in Al2O3-C Refractories for Sliding Gate Applications, Proceedings of the Unified International Technical Conference on Refractories, Salvador, Brazil, October 13 – 16, (2009).
3 Roosen, A.: Tape casting of ceramic green tapes for multilayer device processing, Ceram.Trans., 97, 103 – 121, (1999).
4 Götschel, I., Hayashi, Y., Kakimoto, K.-I., Roosen, A.: Tape casting of Al2O3, MgO, and MgAl2O4 for the manufacture of multilayer composites for refractory applications, Int. J. Appl. Ceram. Tec., 9, [2], 329 – 340, (2012).
5 Green, D.J., Cai, P.Z., Messing, G.L.: Residual stresses in alumina-zirconia laminates, J. Eur. Ceram. Soc., 19, [13 – 14], 2511 – 2517, (1999).
6 Danzer, R., Bermejo, R.: Failure resistance optimisation in layered ceramics desgined with strong interfaces, J. Ceram. Sci. Tech., 1, [1], 15 – 20, (2010).
7 Li, Z., Liu, J., Li, S., Du, H.: Microstructure, mechanical properties and thermal shock resistance of LaPO4-ZrO2, J. Alloy. Compd., 480, [2], 863 – 866, (2009).
8 Ã ström, B.T., Pipes, R.B.: Thermoplastic filament winding with on-line impregnation, J. Thermoplast. Compos., 3, 314 – 324, (1990).
9 Kitaguchi, H., Kumakura, H., Hayashi, T., Fujino, K.: A Bi-2223 layer-winding coil using 540 m tape including a joint inside the winding, IEEE T. Appl. Supercon., 21, [3], 1624 – 1627, (2011)
10 Qiu, J., Hanson, A.J., Sullivan, C.R.: Design of toroidal inductors with multiple parallel foil windings, 2013 IEEE 14th Workshop on Control and Modeling for Power Electronics, COMPEL 2013, art. No. 6626473
11 Roisum, D.R.: The mechanics of winding, TAPPI PRESS, Atlanta, 1994.
12 Lennon, G.E., Martin, J.R., Anderson, C.D.: Single-ply paperboard tube and method of forming same, US Patent US 5586963, 1996
13 Sato, H., Shimizu, S.: Method of manufacturing paper tube, European patent EP 0699518 A3, 1996
14 Rautiainen, P.: Papermaking – part 3, finishing, 2nd edition, Paperija Puu Oy, Helsinki, 2010.
15 Wagner, M., Roosen, A., Oostra, H., Höppener, R., De Moya, M.: Novel low voltage piezoactuators for high displacements, J. Electroceram., 14, [3], 231 – 238, (2005).
16 Scheithauer, U., Slawik, T., Scholl, R., Handke, T., Moritz, T., Baumann, A., Grossmann, H., Michaelis, A.: Spiral winding of ceramic and metallic green tapes, (in German), Keramische Zeitschrift, 64, [1], 35 – 39, (2012).
17 Götschel, I., Gutbrod, B., Travitzky, N., Roosen, A., Greil, P.: Processing of preceramic paper and ceramic green tape derived multilayer structures, Adv. Appl.Ceram., 112, 358 – 365, (2013).
18 EN 623 – 2: Advanced technical ceramics; monolithic ceramics; general and textural properties; part 2: determination of density and porosity, European industry norm, 1993.
19 EN 843 – 2: Advanced technical ceramics. Mechanical properties of monolithic ceramics at room temperature; part 2: determination of Young's modulus, shear modulus and Poisson's ratio, European industry norm, 2007.
20 Feilhauer, R.: Method for the determination of the flexural strength of etched and formed aluminium foils, in German, German patent DE3717159A1, 1988.
21 Roosen, A.: New lamination technique to join ceramic green tapes for the manufacturing of multilayer devices, J. Eur. Ceram. Soc., 21, 1993 – 1996, (2001).
22 Dudczig, S., Aneziris, C.G., Dopita, M., Rafaja, D.: Application of oxide coatings for improved steel filtration with the aid of a metal casting simulator, Adv. Eng. Mater., 15, [12], 1177 – 1187, (2013).
23 Hasselman, D.P.H.: Thermal stress resistance parameters for brittle refractory ceramics: a compendium, Am. Ceram. Soc. Bull., 49, 1033 – 1037, (1970).
Copyright
Göller Verlag GmbH