• Home
  • Contact
  • Login
  • Privacy
  • Imprint

Search

Journal of Ceramic Science and Technology

The Journal of Ceramic Science and Technology publishes original scientific articles on all topics of ceramic science and technology from all ceramic branches. The focus is on the scientific exploration of  the relationships between processing, microstructure and properties of sintered ceramic materials as well as on new processing routes for innovative ceramic materials. The papers may have either theoretical or experimental background. A high quality of publications will be guaranteed by a thorough double blind peer review process.

The Journal is published by Göller Verlag GmbH on behalf of the Deutsche Keramische Gesellschaft (DKG). Edited by Yu-Ping Zeng, Shanghai Institute of Ceramics, Chinese Academy of Sciences, China.

  • Home
  • Early view
  • Articles
    • All articles
    • Recent Articles
    • Early Views
  • Issues
  • Submit an article
  • Guidelines for Referees
  • Guidelines for Authors
  • Open Access
  • Editorial Board
  • Copyright
  • Contact
  • Order journal / article
  • Customer area
  • Terms of Service

Journal Metrics

Web of science
Impact Factor: 1,220
Impact Factor without Journal Self Cites: 1,060
5 Year Impact Factor: 0,818

Scopus
Scimago Journal Rank (SJR):  0,378

 

Prices

Authors
1,300 € Open Access

Print Subscription
62 € per year

view all subscriptions

 

Payment methods

 Credit card

 Invoice

 Wire transfer

 

Articles

All articles  |  Recent articles

A Modelling Approach to Designing Microstructures in Thermal Barrier Coatings

M. Gupta1, P. Nylén1, J. Wigren2

1 University West, 46186 Trollhättan, Sweden
2 Volvo Aero Corporation, 46181 Trollhättan, Sweden

received October 5,2013, received in revised form January 17, 2013, accepted February 14, 2013

Vol. 4, No. 2, Pages 85-92   DOI: 10.4416/JCST2012-00044

Abstract

Thermomechanical properties of Thermal Barrier Coatings (TBCs) are strongly influenced by coating defects, such as delaminations and pores, thus making it essential to have a fundamental understanding of microstructure-property relationships in TBCs to produce a desired coating. Object-Oriented Finite element analysis (OOF) has been shown previously as an effective tool for evaluating thermal and mechanical material behaviour, as this method is capable of incorporating the inherent material microstructure as input to the model. In this work, OOF was used to predict the thermal conductivity and effective Young's modulus of TBC topcoats. A Design of Experiments (DoE) was conducted by varying selected parameters for spraying Yttria-Stabilised Zirconia (YSZ) topcoat. The microstructure was assessed with SEM, and image analysis was used to characterize the porosity content. The relationships between microstructural features and properties predicted by modelling are discussed. The microstructural features having the most beneficial effect on properties were sprayed with a different spray gun so as to verify the results obtained from modelling. Characterisation of the coatings included microstructure evaluation, thermal conductivity and lifetime measurements. The modelling approach in combination with experiments undertaken in this study was shown to be an effective way to achieve coatings with optimised thermo-mechanical properties.

Download Full Article (PDF)

Keywords

Thermal barrier coatings, yttria-stabilised zirconia, OOF, microstructure, thermo-mechanical properties

References

1 Markocsan, N., Nylén, P., Wigren, J., Li, X.-H.: Low thermal conductivity coatings for gas turbine applications, J. Therm. Spray Technol., 16, [5], 498 – 505, (2007).

2 Vassen, R., Stuke, A., Stöver, D.: Recent developments in the field of thermal barrier coatings, J. Therm. Spray Technol., 18, [2], 181 – 186, (2009).

3 Vassen, R., Jarligo, M.O., Steinke, T., Mack, D.E., Stöver, D.: Overview on advanced thermal barrier coatings, Surf. Coat. Technol., 205, 938 – 942, (2010).

4 Vaidya, A., Srinivasan, V., Streibl, T., Friis, M., Chi, W., Sampath, S.: Process maps for plasma spraying of yttria-stabilized zirconia: an integrated approach to design, optimization and reliability, Mater. Sci. Eng., A, 497, 239 – 253, (2008).

5 Mauer, G., Vassen, R., Stöver, D.: Atmospheric plasma spraying of yttria-stabilized zirconia coatings with specific porosity, Surf. Coat. Technol., 204, 172 – 179, (2009).

6 Markocsan, N., Nylén, P., Wigren, J., Li, X.-H., Tricoire, A.: Effect of thermal aging on microstructure and functional properties of zirconia-base thermal barrier coatings, J. Therm. Spray Technol., 18, [2], 201 – 208, (2009).

7 Cao, X.Q., Vassen, R., Stöver, D.: Ceramic materials for thermal barrier coatings, J. Am. Ceram. Soc., 24, 1 – 10, (2004).

8 Curry, N., Donoghue, J.: Evolution of thermal conductivity of dysprosia stabilised thermal barrier coating systems during heat treatment, Surf. Coat. Technol., 209, 38 – 43, (2012).

9 McPherson, R.: The relationship between the mechanism of formation, microstructure and properties of plasma-sprayed coatings, Thin Solid Films, 83, [3], 297 – 310, (1981).

10 Friis, M.: A methodology to control the microstructure of plasma sprayed coatings, Ph. D. Thesis, Lund University, Sweden, (2002).

11 Vassen, R., Träger, F., Stöver, D.: Correlation between spraying conditions and microcrack density and their influence on thermal cycling life of thermal barrier coatings, J. Therm. Spray Technol., 13, [3], 396 – 404, (2004).

12 Sampath, S.: Thermal sprayed ceramic Coatings: fundamental issues and application considerations, Int. J. Mater. Prod. Technol., 35, [3 – 4], 425 – 429, (2009).

13 Dorvaux, J.M., Lavigne, O., Mevrel, R., Poulain, M., Renollet, Y., Rio, C., Modelling the thermal conductivity of thermal barrier coatings. In: Proceedings of the 85th meeting of the AGARD structures and materials panel. NATO-AGARD-R-823, Aalborg, Denmark, 13 – 1 – 13 – 10, (1998).

14 Friis, M., Nylén, P., Persson, C., Wigren, J.: Investigation of particle in-flight characteristics during atmospheric plasma spraying of yttria-stabilized ZrO2: part 1. experimental, J. Therm. Spray Technol., 10, [0], 301 – 310, (2001).

15 Langer, S.A., Fuller Jr., E.R., Carter, W.C.: OOF: an image-based finite-element analysis of material microstructures, Comput. Sci. Eng., 3, [3], 15 – 23, (2001).

16 Reid, A.C.E., Langer, S.A., Lua, R.C., Coffman, V.R., Haan, S.-I., García, R.E.: Image-based finite element mesh construction for material microstructures, Comput. Sci. Eng., 43, [4], 989 – 999, (2008).

17 http://www.ctcms.nist.gov/oof/oof2/ (4th Oct, 2012)

18 Wang, Z., Kulkarni, A., Deshpande, S., Nakamura, T., Herman, H.: Effects of pores and interfaces on effective properties of plasma sprayed zirconia coatings, Acta Mater., 51, [18], 5319 – 5334, (2003).

19 Jadhav, A.D., Padture, N.P., Jordan, E.H., Gell, M., Miranzo, P., Fuller Jr., E.R.: Low-thermal-conductivity plasma-sprayed thermal barrier coatings with engineered microstructures, Acta Mater., 54, [12], 3343 – 3349, (2006).

20 Gupta, M., Nylén, P.: Design of low thermal conductivity thermal barrier coatings by finite element modelling. In: Proceedings of the twenty fourth international conference on surface modification technologies. T.S. Sudarshan, E. Beyer, and L.-M Berger, ed., Dresden, Germany, (2010).

21 Jadhav, A.D., Padture, N.P.: Mechanical properties of solution-precursor plasma-sprayed thermal barrier coatings, Surf. Coat. Technol., 202, 4976 – 4979, (2008).

22 Azarmi, F., Coyle, T., Mostaghimi, J.: Young's modulus measurement and study of the relationship between mechanical properties and microstructure of air plasma sprayed alloy 625, Surf. Coat. Technol., 203, 1045 – 1054, (2009).

23 Nakamura, T., Liu, Y.: Determination of nonlinear properties of thermal sprayed ceramic coatings via inverse analysis, Int. J. Solids Struct., 44, [6], 1990 – 2009, (2007).

24 Liu, Y., Nakamura, T., Srinivasan, V., Vaidya, A., Gouldstone, A., Sampath, S.: Non-linear elastic properties of plasma-sprayed zirconia coatings and associated relationships with processing conditions, Acta Mater., 55, [14], 4667 – 4678, (2007).

25 Liu, Y.J., Nakamura, T., Dwivedi, G., Valarezo, A., Sampath, S.: Anelastic behavior of plasma-sprayed zirconia coatings, J. Am. Ceram. Soc., 91, [12], 4036 – 4043, (2008).

26 Dwivedi, G., Nakamura, T., Sampath, S.: Controlled introduction of anelasticity in plasma-sprayed ceramics, J. Am. Ceram. Soc., 94, [s1], s104 – s111, (2011).

27 Vassen, R., Kerkhoff, G., Stöver, D.: Development of a micromechanical life prediction model for plasma sprayed thermal barrier coatings, Mater. Sci. Eng., A, 303, 100 – 109, (2001).

28 Matejicek, J., Sampath, S.: In situ measurement of residual stresses and elastic moduli in thermal sprayed coatings part 1: apparatus and analysis, Acta Mater., 51, 863 – 872, (2003).

29 Tano, I., Gupta, M., Curry, N., Nylén, P., Wigren, J.: Relationships between coating microstructure and thermal conductivity in thermal barrier coatings – A modelling approach. In: Thermal spray: Global solutions for future application. DVS – German Welding Society, and ASM International, Singapore, (2010).

30 Curry, N., Markocsan, N., Li, X.-H., Tricoire, A., Dorfman, M.: Next generation thermal barrier coatings for the gas turbine industry, J. Therm. Spray Technol., 20, [1 – 2], 108 – 115, (2011).

Copyright

Göller Verlag GmbH

Special and Topcial Issues

Topical Issue, 3/2017
Guest Editors:
Waltraud M. Kriven and Gregor J. G. Gluth
Geopolymers

Special Issue, 1/2017
Guest Editor:
Alexander Michaelis
6th International Congress on Ceramics (ICC6)

Topical Issue, 2/2016
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advan-ced steel technologies; A challenge for refractory materials and systems.

Topcial Issue, 4/2015
Low Temperature Co-fired Ceramics - LTCC

Topcial Issue, 2/2015
Status of Additive Manufacturing with Ceramics

Topical Focus, 4/2014
Materials Processing Science with Lasers as Energy Sources

Topical Issue, 2/2014
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advanced steel technologies; A challenge for refractory materials and systems.

Special Issue, 2/2013
Guest Editor:
Alexander Michaelis
Ceramic Materials and Components for Energy and Environmental Applications

Topical Issue, 1/2013
Ceramic Processing Science with Lasers as Energy Sources

Printed version

jcst 2015 02 cover

Order journal subscription
 

© 2009-2017 Göller Verlag GmbH