Articles
All articles | Recent articles
Selective Laser Sintering as an Additive Manufacturing Method for Manufacturing Ceramic Components
M. Ahlhelm, H.-J. Richter, K. Haderk
Fraunhofer Institute for Ceramic Technologies and Systems (IKTS) Winterbergstrasse 28, 01277 Dresden, Germany
received June 29, 2012, received in revised form November 19, 2012, accepted December 03, 2012
Vol. 4, No. 1, Pages 33-40 DOI: 10.4416/JCST2012-00024
Abstract
Selective Laser Sintering (SLS) offers the advantage of directly manufacturing complex-shaped parts without the uneconomic loss of material so common when conventional manufacturing methods are applied. Originating from the laser sintering of polymers, lots of research has been conducted on advanced materials like metals and ceramics. In recent years the Fraunhofer IKTS has conducted research on the laser sintering of SiC and different hydroxyapatite (HAp) powders. The HAp powders have been characterized based on their laser sintering ability with the variation of process parameters like spreading behavior, different grain shape and size, hatch clearance, etc. More elaborate research has been conducted concerning the laser sintering of SiSiC components. After infiltration and pyrolysis of laser-sintered SiC parts, the resulting SiSiC components showed similar mechanical characteristics to those of conventionally processed SiSiC components. Different complex geometries were realized e.g. a 120-mm honeycomb-structured mirror support model (wall thickness of 1 mm, for aerospace applications) and a small turbine rotor (minimal wall thickness of 0.3 mm) as a demonstrator part for automotive components. A laser mirror with integrated cooling channels for application in movable beam arms for laser material processing was also manufactured. Another successfully generated SiSiC component is an injection molding tool insert (ca. 35 x 30 mm; diameter x height) with a complex-structured surface and inner cooling channels. The next steps will be towards research dealing with more complex designs and other ceramics as well as metal-ceramic hybrids.
Download Full Article (PDF)
Keywords
Selective Laser Sintering (SLS), ceramic, silicon carbide, hydroxyapatite
References
1 US 4 247 508
2 US 4 938 816
3 Kruth J.-P. et al.: Mechanisms in selective laser sintering and selective laser melting, Rapid Prototyping J., 11 (1), 26 – 36, (2005).
4 Löschau, W. et al.: Prototyping of complex-shaped parts and tools of Si/SiC-ceramics by selective laser sintering, Ind. Ceram., 20 (2), 95 – 96, (2000).
5 Löschau, W. et al., DE 197 30 739 C2
6 Lee, I.S.: Rapid full densification of alumina-glass composites fabricated by a selective laser sintering process, J. Mater. Sci. Lett.., 17 (22), 1907 – 1911, (1998).
7 Görke, R., Krause, T., Günster, J., Ries, C., Heinrich, J.G.: Laser-assisted sintering of porcelain, Ceram. Trans., 108 (Innovative Processing and Synthesis of Ceramics, Glasses, and Composites III), 91 – 96, (2000).
8 Harlan, N., Park, S.-M., Bourell, D.L., Beaman, J.J.: Selective laser sintering of zirconia with micro-scale features, Sol. Freeform Fabric., 297 – 310, (1999).
9 Goodridge, R.D., Lorrison, J.C., Dalgarno, K.W., Wood, D.J.: Comparison of direct and indirect selective laser sintering of porous apatite mullite glass ceramics, Glass Technol., 45, (2) 94 – 96, (2004).
10 Fischer, H., Wilkes, J., Bergmann, C., Kuhl, I., Meiners, W., Wissenbach, K., Poprawe, R., Telle, R.: Bone substitutes implants made of TCP/glass composites using selective laser melting technique, cfi/Ber. DKG, 83, 13, 57 – 60, (2006).
11 Heymadi, U., McAlea, K.: Selective laser sintering of metal molds, the rapid tool process, Sol. Freeform Fabric., 97 – 104, (1996).
12 Das, S. et al.: Direct SLS processing for production of cermet turbine sealing components, Mater. Manuf. Processes, 13 (2), 241 – 261, (1998).
13 Jiacheng, G., Yaping, Z., Mingfei, C.: Reacting composing HAp by laser sintering; International Symposium on the Science and Technology of Sintering, 6, 313 – 318, (1995).
14 Lee, G., Barlow, J.W.: Selective laser sintering of calcium phosphate powders, Sol. Freeform Fabric., 191 – 197, (1994).
15 Vail, N.K., Swain, L.D., Fox, W.C., Aufdemorte, T.B.; Lee, G., Barlow, J.W.: Materials for biomedical applications, Sol. Freeform Fabric., 621 – 628, (1998).
16 Cruz, F., Simoes, J.F.A., Coole, T.J., Bocking, C.: Fabrication of customized bioceramic implants using selective laser sintering; Third National Conference on Rapid Prototyping, Tooling and Manufacturing, High Wycombe, GB, ISBN 1 – 86058 – 374 – 1, 63 – 70, (2002).
17 Chua, C.K., Leong, K.F., Tan, K.H., Wiria, F.E., Chea, C.M.: Development of tissue scaffolds using selective laser sintering of polyvinyl alcohol/hydroxyapatite biocomposite for craniofacial and joint defects; J. Mater. Sci. - Mater. M., 15, 1113 – 1121, (2004).
18 Tan, K.H. et al.: Selective laser sintering of biocompatible polymers for applications in tissue engineering, Bio-Med. Mater. Eng., 15, 113 – 124, (2005).
19 Tan, K.H. et al.: Scaffold development using selective laser sintering of polyetheretherketone-hydroxyapatite biocomposite blends; Biomaterials, 24, 3115 – 3123, (2003).
20 Lenk, R., Nagy, A., Richter, H.-J., Techel, A.: Material development for laser sintering of silicon carbide, cfi/Ber. DKG, 83, 13, 41 – 43, (2006).
21 Wohlert, M., Bourell, D.: Rapid prototyping of Mg/SiC composites by a combined SLS and pressureless infiltration process, Sol. Freeform Fabric., 79 – 87, (1996).
22 Hagedorn, Y.-C.,Wilkes, J., Meiners, W., Wissenbach K., Poprawe, R.: Net-shaped high performance oxide ceramic parts by selective laser melting, Physics Procedia, 5, 587 – 594, (2010).
23 Goodridge, R.D. et al.: Biological evaluation of an apatite-mullite glass-ceramic produced via selective laser sintering, Acta Biomat., 3, 221 – 231, (2007).
24 Stierlen, P.: Rapid Prototyping of ceramics – development of a process for the production of reaction-bonded SiSiC-prototypes (in German), PhD-Thesis, University Stuttgart, Shaker Verlage Aachen (2002).
25 Richter, H.-J., Ahlhelm, M., Haderk, K.: Process and material development for laser sintering of silicon carbide, Conference paper for 1st DDMC, Berlin 2012.
26 DE 19730739C2.
27 Techel, A. et al.: Laser Sintering of Complex-Shaped Ceramic Prototypes, Pacific International Conference on Applications of Lasers and Optics, Melbourne, (2004)
28 Streek, A., Regenfuss, P., Ebert, R., Exner, H.: Laser micro sintering – upgrade of the technology, Laser Institute of America [Publication], 102, 1140 – 1147, (2009).
29 Regenfuss, P. et al., Laser micro sintering of ceramic materials, part 2, Interceram, 57 (1), 6 – 9, (2008).
Copyright
Göller Verlag GmbH