Laser Synthesis of Al2TiO5 Ceramics from Al2O3-TiO2 Powder Mixtures

M. Vlasova1, B. Sosa Coeto1, M. Kakazey1, P. A. Marquez Aguilar1, 1, A. Escobar Martinez1, V. Stetsenko2, A. Bykov2

1 Center of Investigation in Engineering and Applied Sciences of the Autonomous University of the State of Morelos (CIICAp-UAEMor), Av. Universidad, 1001, Cuernavaca, Mexico.
2 Institute for Problems of Materials Science, National Academy of Sciences of Ukraine, 3, Krzhyzhanovsky St., Kiev, 252680, Ukraine

received January 25, 2012, received in revised form February 26, 2012, accepted March 21, 2012

Vol.3, No.2, Pages 61-68   DOI: 10.4416/JCST2012-00005

Abstract

The phase formation process in the zone of laser irradiation of Al2O3-TiO2 compacts with different contents of components has been investigated with XRD, electron microscopy, and atomic force microscopy methods. The distinctive feature of laser synthesis is the simultaneous formation of α- and β-Al2TiO5, which is caused by the non-uniform heating of the material in the irradiation zone. The motion of the eutectic melt under the action of hydrodynamic forces is the motive force for texturing of precipitating crystalline phases during fast cooling. The degree of texturing of Al2O3 and Al2TiO5 crystallites depends on the amount of the formed eutectic melt.

Purchase Full Article or get a Subscription

Keywords

Al2O3, TiO2, laser treatment, Al2TiO5

References

1 Han, Ch., Selb, D.: Improving aluminium-titanate ceramics, (in German), Sprechsaal, 118, [12], 1157 – 1166, (1985).

2 Ishitsuka, M., Sato, T., Endo, T., Shimada, M.: Synthesis and thermal stability of aluminium titanate solid solutions, J. Am. Ceram. Soc., 70 [2], 69 – 71, (1987).

3 Thomas, H.A., Stevens, R.: Aluminium titanate – A literature review, part 1: Microcracking phenomena, Br. Ceram. Trans. J., 88, 144 – 151, (1989).

4 Kim, I.J., Kwak, H.S.: Thermal shock resistance and thermal expansion behaviour with composition and microstructure of Al2TiO5 ceramics, Can. Metall. Quart., 39 [4], 387 – 395, (2000).

5 Sekar, M.M.A., Patil, K.C.: Synthesis and properties of tialite, β-Al2TiO5, Brit. Cer. T., 93 [4], 146 – 9, (1994).

6 Oo, Z., Low, I.M.: Indentation responses of functionally-graded Al2TiO5-based ceramics, in: Advanced materials research, 239 – 242, 171 – 174, 2011. Eds. Zhong Cao, Xueqiang Cao, Lixian Sun, Yinghe He, DOI 10.4028/www.scientific.net/AMR.239 – 242.171.

7 Zaharescu, M., Crisan, M., Preda, M., Fruth, V., Preda, S.: Al2TiO5-based ceramics obtained by hydrothermal processes, J. Optoelectron. Adv. M., 5, [5], 1411 – 1416, (2003).

8 Neppolian, B., Wang, Q., Jung, H., Choi, H.: Ultrasonic-assisted sol-gel method of preparation of TiO2 nano-particles: Characterization, properties and 4-chlorophenol removal application, Ultrason. Sonochem., 15, [4], 649 – 658, (2008).

9 Camaratta, R., Acchar, W., Bergmann, C.P.: Phase transformations in the Al2O3/TiO2 system and metastable phase formation at low temperatures, Rev. Adv. Mater. Sci., 27, 64 – 68, (2011).

10 Stanciu, L., Groza, J.R., Stoica, L., Plapcianu, C.: Influence of powder precursors on reaction sintering of Al2TiO5, Scripta Mater., 50, 1259 – 1262, (2004).

11 Nagano, M., Nagashima, S., Maeda, H., Kato, A.: Sintering behavior of Al2TiO5 base ceramics and their thermal properties, Ceram. Int., 25 [8], 681 – 687, (1999).

12 Norberg, S.T., Ishizawa, N., Hoffmann, S., Yoshimura, M.: Redetermination of β-Al2TiO5 obtained by melt casting, Acta Crystallogr., Section E61, i160 – i162, (2005).

13 Huang, C.-L., Wang L.-J.: Microwave dielectric properties of sintered alumina using nano-scaled powders of a alumina and TiO2, J. Am. Ceram. Soc., 90 [5], 1487 – 1493, (2007).

14 Hoffmann, S., Norberg, S.T., Yoshimura, M.: Melt Synthesis of Al2TiO5 Containing composites and reinvestigation of the phase diagram Al2O3-TiO2 by powder x-ray diffraction, J. Electroceram., 16, N. 4, 327 – 330, (2006).

15 Duan, R.-G., Zhan, G.-D., Kuntz, J. D., Kear, B.H., Mukherjee, A.K.: Spark plasma sintering (SPS) consolidated ceramic composites from plasma-sprayed metastable Al2TiO5 powder and Nano-Al2O3, TiO2, and MgO powders, Mater. Sci. Eng. A, 373, [1 – 2], 180 – 186, (2004).

16 LLorca, J., Orera, V.M.: Directionally solidified eutectic ceramic oxides, Prog. Mater. Sci., 51, 711 – 809, (2006).

17 Orera, V.M., Merino, R.I., Pardo, J.A., Larrea, A.A., Peña, J.I., Gonzalez, C., Poza, P., Pastor, J.Y., LLorca, J.: Microstructure and physical properties of some oxide eutectic composites processed by directional solidification, Acta Mater., 48 [18/19], 4683 – 4689, (2000).

18 Su, H, Zhang, J., Deng, Y., Liu, L., Fu, H.: A modified preparation technique and characterization of directionally solidified Al2O3/Y3Al5O12 eutectic In Situ composites, Scripta Mater., 60, [2], 362 – 365, (2009).

19 Berger, M.-H., Sayir, A.: Directional solidification of Al2O3-Al2TiO5 system, J. Eur. Ceram. Soc., 28, 2411 – 2419, (2008).

20 Vlasova, M., Kakazey, M., Márquez Aguilar, P.A.: Microstructural Evolution in α-Al2O3 Compacts during laser irradiation, Chapter in book: Advances in Ceramics. Synthesis and Characterization, Processing and Specific Application, Ed. Costas Sikalidis//Niksa Mandic . ISBN 978 – 953 – 307 – 505 – 1. INTECH - Open Access Publisher, 2011. pp. 393 – 420.

21 Heinrich, J.G., Gahler, A., Günster, J., Schmücker, M., Zhang, J., Jiang, D., Ruan, M.: Microstructural evolution during direct laser sintering in the Al2O3-SiO2 system, J. Mater. Sci., 42, 5307 – 5311, (2007).

22 Toropov, N.A.: State Diagrams of Silicate Systems, 2nd ed., Leningrad, Nauka, 1969.

23 Butting, E.N.: Phase equilibrium in the system TiO2, TiO2-SiO2 and TiO2-Al2O3, Bull. Stand. J. Res., 11, 725, (1933).

24 Buscaglia, V., Nanni, P.: Decomposition of Al2TiO5 and Al2(1-x)MgxTi(1+x)O5 ceramics, J. Am. Ceram. Soc., 81, [10], 2645 – 53, (1998).

25 Venkataraman, R., Singh, P., Krishnamurthy, R.: Enhanced alpha phase stability during plasma spraying of alumina-13 mol% titania, J. Am. Ceram. Soc., 89 [2], 734 – 736, (2006).

26 Zaĭkin, A.E., Katulin, V.A., Levin, A.V., Petrov, A.L.: Hydrodynamic processes in a melt bath under laser-arc interaction conditions, Sov. J. Quantum Electron., 21, [6], 635 – 639, (1991).

27 Lu, Y., Chen, S.C.: Nanopatterning of a silicon surface by near-field enhanced laser irradiation, Nanotechnology, 14, [4], 505 – 508, (2003).

28 Alaverdyan, R.B., Grigoryan, A.M., Chilingaryan, Yu. S.: Convection in relatively thin layers of nematic liquid crystals, J. Contemp. Phys. – Arme., 43, [1], 19 – 22, (2008).

Copyright

Göller Verlag GmbH

 

Printed version

jcst_cover_2013-1

Order journal subscription

© 2009-2013 Göller Verlag GmbH