Laser-Fused Transparent Microspheres with the Eutectic Composition Al2O3-Y2O3-ZrO2 (AYZ)

C. Oelgardt1, J. Günster2, J. G. Heinrich3

1 Clausthal University of Technology, Institute of Nonmetallic Materials, Department for Engineering Ceramics, 38678 Clausthal-Zellerfeld, Germany
2 BAM – Federal Institute for Materials Research and Testing, Division 5.4 – Advanced Ceramics, 12203 Berlin, Germany
3 Clausthal University of Technology, Institute of Nonmetallic Materials, Department for Engineering Ceramics, 38678 Clausthal-Zellerfeld, Germany

received March 9, 2011, , accepted March 22, 2011

Vol.2, No.2, Pages 103-110   DOI: 10.4416/JCST2011-00010

Abstract

Transparent microspheres with the eutectic composition 65 Al2O3-16 Y2O3-19 ZrO2 (mol%) have been produced by laser fusing with a CO2 laser. The influence of the starting material – not pre-calcined and pre-calcined – as well as the laser power on the resulting microspheres – was investigated. After fabrication, the microspheres were analyzed by means of XRD to quantify the amorphous content of the spheres as well as to identify the residual crystalline phases, with a laser granulometer to measure the particle sizes of the starting material and the resulting microspheres, with DSC to characterize the glass transition temperature and crystallization behavior, and with SEM to investigate the microstructure of the microspheres. The laser-treated materials consist of transparent and opaque beads as well as sintered particles. The amorphous amount in the samples was detected to be ∼ 85 %. Based on these results transparent beads were collected and annealed over a range of temperatures to analyze the crystallization behavior.

Purchase Full Article or get a Subscription

Keywords

Eutectic ceramics, Al2O3-Y2O3-ZrO2, laser processing, crystallization behavior, microstructure

References

1 Ikesue, A., Kamata, K.: Microstructure and optical properties of hot isostatically pressed Nd:YAG ceramics, J. Am. Ceram. Soc., 79, 1927 – 1933, (1996).

2 Gilde, G., Patel, P., Patterson, P., Blodget, D., Duncan, D., Hahn, D.: Evaluation of hot pressing and hot isostatic pressing parameters on the optical properties of spinel, J. Am. Ceram. Soc., 88, 2747 – 2751, (2005).

3 Itatani, K., Tsujimoto, T., Kishimoto, A.: Thermal and optical properties of transparent magnesium oxide ceramics fabricated by post hot-isostatic pressing, J. Eur. Ceram. Soc., 26, 639 – 645, (2006).

4 Salman, S.M., Salama, S.N., Abo-Mosallam, H.A.: Crystallization behaviour and properties of multicomponent strontium-containing lithia calcia silicate glasses, Ceram. Int., 36, 2307 – 2314, (2010).

5 El-Kheshen, A.A., Zawrha, M. F.: Sinterability, microstructure and properties of glass/ceramic composites, Ceram. Int., 29, 251 – 257, (2003).

6 Alekseeva, I., Dymshiths, O., Tsenter, M., Zhilim, A., Golubkov, V., Denisov, I., Skoptsov, N., Malyarevich, A., Yumashev, K.: Optical applications of glass-ceramics, J. Non-Cryst. Sol., 356, 3042 – 3058, (2010).

7 Boutarfaia, A., Legouera, M., Poulain, M.: Glass formation and crystallization kinetics in a multicomponent fluoride glass, J. Non-Cryst. Sol., 291, 176 – 180, (2001).

8 Araki, S., Yoshimura, M.: Transparent nano-composite ceramics by annealing of amorphous phase in the HfO2-Al2O3-GdAlO3 system, Int. J. Appl. Ceram. Technol., 1, 155 – 160, (2004).

9 MacDowell, J.F., Beall, G.H.: Immiscibility and crystallization in Al2O3-SiO2 glasses, J. Am. Ceram. Soc., 52, 17 – 25, (1969).

10 Claussen, N., Lindemann, G., Petzow, G.: Rapid solidification in the Al2O3 - ZrO2 system, Ceram. Int., 9, 83 – 86, (1983).

11 Thorne, D.J.: Glass formation in refractory oxide systems based on alumina, Proc. Br. Ceram. Soc., 14, 131 – 145, (1969).

12 Takamori, T., Roy, R.: Rapid crystallization of SiO2-Al2O3 glasses, J. Am. Ceram. Soc., 56, 639 – 644, (1973).

13 Rosenflanz, A., Frey, M., Endres, B., Anderson, T., Richards, E., Schardt, C.: Bulk glasses and ultrahard nanoceramics based on alumina and rare-earth oxides, Nature, 430, 761 – 764, (2004).

14 Rosenflanz, A., Frey, M., Endres, B., Anderson, T., Richards, E., Schardt, C.: Bulk glasses and glass-ceramics based on Al2O3, their processing methods and properties, Glass Sci. Technol. C, 78, 27 – 32, (2005).

15 Prnová, A., Karell, R., Galusek, D.: Y2O3-Al2O3 binary glass microspheres: Synthesis and characterisation, Adv. Mat. Res., 39 – 40, 189 – 192, (2008).

16 Prnová, A., Karell, R., Galusek, D.: The preparation of binary Al2O3-Y2O3 glass microspheres by flame synthesis from powder oxide precursors, Ceramics - Silikáty, 52, 109 – 114, (2008).

17 Samant, A.N., Dahotre, N.B.: Laser machining of structural ceramics - A review, J. Eur. Ceram. Soc., 29, 969 – 993, (2009).

18 Bertrand, P., Bayle, F., Combe, C., Goeuriot, P., Smurov, I.: Ceramic components manufacturing by selective laser sintering, Appl. Surf. Sci., 254, 989 – 992, (2007).

19 Ester, F.J., Merino, R.I., Pastor, J.Y., Martin, A., LLorca, J.: Surface modification of Al2O3-ZrO2(Y2O3) eutectic oxides by laser melting: processing and wear resistance, J. Am. Ceram. Soc., 91, 3552 – 3559, (2008).

20 Gahler, A., Heinrich, J.G., Kawanowa, H., Schwertfeger, F., Günster, J.: Three-dimensional laser surface sintering of SiO2 green bodies, Int. J. Appl. Ceram. Technol., 3, 331 – 335, (2006).

21 Hoon Kim, S., Sohn, I.-B., Jeong, S.: Ablation characteristics of aluminium oxide and nitride ceramics during femtosecond laser micromachining, Appl. Surf. Sci., 225, 9717 – 9720, (2009).

22 Sola, D., Escartin, A., Cases, R., Pena, J.I.: Laser ablation of advanced ceramics and glass-ceramic materials: Reference position dependence, Appl. Surf. Sci., 257, 5413 – 5419, (2011).

23 Tian, X., Günster, J., Melcher, J., Li, D., Heinrich, J.G.: Process parameters analysis of direct laser sintering and post treatment of porcelain components using Taguchi's method, J. Eur. Ceram. Soc., 29, 1903 – 1915, (2009).

24 Gahler, A., Heinrich, J.G.: Direct laser sintering of Al2O3-SiO2 dental ceramic components by layer-wise slurry deposition, J. Am. Ceram. Soc., 89, 3076 – 3080, (2006).

25 Günster, J., Engler, S., Heinrich, J.G., Schwertfeger, F.: A novel route for the production of ultra pure SiO2 crucibles, Glass Sci. Technol. , 78, 18 – 22, (2005).

26 Lakiza, S.M.: Directionally solidified eutectics in the Al2O3-ZrO2-Ln8Y)2O3 systems (Review), Powder Metall. Met. Ceram., 48, 42 – 59, (2009).

27 Pastor, J.Y., LLorca, J., Martín, A., Pena, J.I., Oliete, P.B.: Fracture toughness and strength of Al2O3-Y3Al5O12 and Al2O3-Y3Al5O12-ZrO2 directionally solidified eutectic oxides up to 1900 K, J. Eur. Ceram. Soc., 28, 2345 – 2351, (2008).

28 Su, H., Zhang, J., Deng, Y., Liu, L., Fu, H.: A modified preparation technique and characterization of directionally solidified Al2O3/Y3Al5O12 eutectic in situ composites, Scripta mater., 60, 362 – 365, (2009).

29 Oliete, P.B., Pena, J.I., Larrea, A., Orera, V.M., LLorca, J., Pastor, J.Y., Martin, A., Segurado, J.: Ultra-high-strength nanofibrillar Al2O3-YAG-YSZ eutectics, Adv. Mater., 19, 2313 – 2318, (2007).

30 Westphal, T., Füllmann, T., Pöllmann, H.: Rietveld quantification of amorphous portions with an internal standard - Mathematical consequences of the experimental approach, Powder Diffr., 24, 239 – 243, (2009).

31 Oelgardt, C., Anderson, J., Heinrich, J.G., Messing, G.L.: Sintering, microstructure and mechanical properties of Al2O3-Y2O3-ZrO2 (AYZ) eutectic composition ceramic microcomposites, J. Europ. Ceram. Soc., 30, 649 – 656, (2010).

32 Herziger, G., Loosen, P.: Materials processing with lasers (in German), Hanser Verlag, Munich - Vienna (1993).

33 Wilding, M.C., McMillan, P.F.: Polyamorphic transition in yttria-alumina liquids, J. Non-Cryst. Sol., 293 – 295, 357 – 365, (2001).

Copyright