ArticlesAll articles | Recent articles Methods of Quantification of the Internal Structures of Spray Granules S. Höhn, S. Eckhard, M. Fries, B. Matthey, M. Herrmann, A. Michaelis Fraunhofer Institute for Ceramic Technologies and Systems, Winterbergstrasse 28, 01277 Dresden, Germany received January 20, 2011, , accepted February 28, 2011 Vol.2, No.2, Pages 75-88 DOI: 10.4416/JCST2011-00003 AbstractGranules for die pressing applications prepared by means of spray drying need to possess specific properties defined by the end-application. The internal structure of the granules is therefore an important quality-determining property because it influences both the processing properties of the loose granules and the defect distribution in the sintered ceramic part. In this paper, an optimized, artifact-free, gentle and reproducible preparation method based on ion beam technology for exposing the internal granule structures is presented. Model Al2O3 granules are used to demonstrate the possibilities for imaging via high-resolution scanning electron microscopy and quantification of the granules in terms of porosity as well as particle and additive distribution. KeywordsGranule, microstructure quantification, ion beam preparation, porosity, particle distance References1 Salmang, H., Scholze, H.: Ceramics (in German), Springer Verlag, Berlin-Heidelberg, (2007). 2 Soottitantawat, A., Peigney, J., Uekaji, Y, Yoshii, H., Furuta, T., Ohgawara, M., Linko, P.: Structural analysis of spray-dried powders by confocal laser scanning microscopy, Asia-Pac. J. Chem. Eng., 2, [1], 41-46, (2007). 3 Walton, D.E., Mumford, C.J.: Spray dried products – Characterization of particle morphology, Chem. Eng. Res. and Design, 77, [1], 21-38, (1999). 4 Masters, K.: Spray Drying in Practice, SprayDryConsult International ApS, Charlottenlund, (2002). 5 Walker, W.J., Reed, J.S., Verma, S.K.: Influence of slurry parameters on the characteristics of spray-dried granules, J. Am. Ceram. Soc., 82, [7], 1711-1719, (1999). 6 Fries, M.: Product design of ceramic spray granulates for uniaxial press compaction to large-size components (in German), Doctorial Dissertation, Techn. Univ. Bergakademie Freiberg, (2008). 7 Hotta, T., Nakahira, K., Naito M., Shinohara, N., Okumiya, M., Uematsu, K.: Origin of the strength change of silicon nitride ceramics with the alteration of spray drying conditions. J. Eur. Ceram. Soc., 21, [5], 603-610, (2001). 8 Bertrand, G., Filiatre, C., Mahdjoub, H., Fossy, A., Coddet, C.: Influence of slurry characteristics on the morphology of spray-dried alumina powders, J. Eur. Ceram. Soc., 23, [2], 263-27, (2003). 9 Bertrand, G., Roy, P., Filiatre, C., Coddet, C.: Spray-dried ceramic powders: A quantitative correlation between slurry characteristics and shape of granules, Chem. Eng. Sci., 60, [1], 95-102, (2005). 10 Lukasiewicz, S.J.: Spray-drying ceramic powders, J. Am. Ceram. Soc., 72, [4], 617-624, (1989). 11 Abe, H., Naito, M., Hotta, T., Kamiya, H., Uematsu, K.: Pore defects related to slurry character and their relevance to strength distribution in alumina ceramics, Powd. Techn., 134, [1-2], 58-64, (2003). 12 Tsubaki, J., Yamakawa, H., Mori, T., Mori, H.: Optimization of granules and slurries for press forming, J. Ceram. Soc. Japan, 110, [10], 894-898, (2002). 13 Shinoharaa, N., Okumiyaa, M., Hottab, T., Nakahirab, K., Naitob, M., Uematsu, K.: Variation of the microstructure and fracture strength of cold isostatically pressed alumina ceramics with the alteration of dewaxing procedures, J. Eur. Ceram. Soc., 20, [7], 843-849, (2000). 14 Yu, Y., Wang, J.: Effect of X-ray irradiation on starch granule structure and physicochemical properties of rice, Food Res. Intern., 40, 297-303, (2007). 15 Baklouti, S., Chartier, T., Baumard, J.F.: Binder distribution in spray-dried alumina agglomerates, J. Eur. Ceram. Soc., 18, [14], 2117-2121, (1998). 16 Tanaka, S., Chia-Pin, C., Kato, Z., Uematsu, K.: Effect of internal binder on microstructure in compacts made from granules, J. Eur. Ceram. Soc., 27, [2-3], 873-877, (2007). 17 Komlev V.S., Barinov, S.M., Giradin, E., Oscarsson, S., Rosengren, A., Rustichelli, F., Orlovskii, V.P.: Porous spherical hydroxyapatite and fluorhydroxyapatite granules: processing and characterization, Sci. and Techn. of Adv. Mat., 4, [6], 503-508, (2003). 18 Wang, S., Yu, J., Zhu, Q., Yu, J., Jin, F., Granular structure and allomorph position in C-type Chinese yam starch granule revealed by SEM, C CP/MAS NMR and XRD, Food Hydrocolloids, 23, [2], 426-433, (2009). 19 Uematsu, K., Kim, J.-Y., Miyashita, M., Uchida, N., Saito, K.: Direct Observation of Internal Structure in Spray-Dried Alumina Granules, J. Am. Ceram. Soc., 73, [8], 1555-1557, (1990). 20 Kim, J.-Y., Inoue, M., Kato, Z., Uchida, N., Saito, K., Uematsu, K.: Direct observation of internal structure in spray-dried yttria-doped zirconia granule, J. Mat. Sci., 26, [8], 2215-2218, (1991). 21 Zhang, Y., Suga, T., Kawasaki, K., Tang, X.X., Uchida, N., Uematsu, K.: Effect of PVA Adsorption on Binder Segregation during Drying, J. Am. Ceram. Soc., 79, [2], 435-440, (1996). 22 Uematsu, K., Ito, H., Zhang, Y., Uchida, N.: Novel characterization method for the processing ceramics by polarized light microscope with liquid immersion technique, Cer. Trans., Am. Ceram. Soc., 54, 83-89, (1995). 23 Uematsu, K., Saito, M.: Liquid immersion technique coupled with IR microscopy for direct observation of internal structure of ceramic powder compact – with alumina as an example, J. Mat. Res., 14, 4463-4465, (1999). 24 Saito, Y., Tanaka, S., Uchida, N., Uematsu, K.: CLSM for Ceramic Green Microstructure, J. Am. Ceram. Soc. Bull., 81, [1], 35-38, (2002). 25 Appoloni, C.R., Macedo, I., Fernandes, C.P.; Philippi, P.C.: Characterization of porous microstructure by x-ray microtomography, X-Ray Spectr., 31, [2], 124-127, (2002). 26 Farber, L., Tardos, G., Michaels, J.N.: Application of X-ray Micro-Tomography to Study the Morphology and Porosity of Pharmaceutical Granules, Microsc. Microanal., 8, [2], 784-785, (2002). 27 Farber, L., Tardos, G., Michaels, J.N.: Use of X-ray tomography to study the porosity and morphology of granules. Powd. Techn., 132, [1], 57-63, (2003). 28 Salvo, L., Cloetens, P., Maire, E., Zabler, S., Blandin, J.J., Buffiere, J.Y., Ludwig, W., Boller, E., Bellet, D., Josserond, C.: X-ray microtomography – an attractive characterisation technique in materials science, Nucl. Instr. Meth. Phys. Res., B200, 273-286, (2003). 29 Rahmanian, N., Ghadiri, M., Jia, X., Stepanek, F.: Characterisation of granule structure and strength made in a high shear granulator, Powd. Techn., 192, [2], 184-194, (2009). 30 Herrmann, M., Schulz, I., Bales, A., Sempf, K., Höhn, S.: "Snow flake" structures in silicon nitride ceramics – Reasons for large scale optical inhomogeneities, J. Eur. Cer. Soc., 28, [5], 1049-1056, (2008). 31 Baumann, A., Brieseck, M., Höhn, S., Moritz, T., Lenk, R.: Developments in Multi-Component Powder Injection Moulding of Steel-Ceramic Compounds using Green Tapes for Inmould Label Process, Powd. Inj. Mold. Int., 2, [1], 55-58, (2008). 32 Mannschatz, A., Höhn, S., Moritz, T.: Powder-binder-separation in injection moulded green parts, J. Eur. Cer. Soc., 30, [14], 2827-2832, (2010). 33 Grove, W.R.: LXXIX. On the Electro-Chemical Polarity of Gases. Phil. Mag., 4, [28], 498-514, (1852). 34 Plücker, J.: On the influence of magnets on electrical discharges in dilute gases (in German), Ann. Phys., 179, [1], 88-106, (1858). 35 Davies, S.T.: Ion beam milling of microelectronic components (in German), Feinwerkt. u. Messt., 95, 243-244, (1987). 36 Liebel, G.: Ion beam etching – a reliable method for the production of microstructures (in German), Feinwerkt. u. Messt., 95, 436-440, (1987). 37 Seliger, R.L., Ward, J.W., Wang, V., Kubena, R.L.: A high-intensity scanning ion probe with submicrometer spot size, Appl. Phys. Lett., 34, [5], 310-312, (1979). 38 Wechsung, R., Aberle, L.: A penning ion source with even beam profile (in German), Vakuum-Techn., 24, [8], 217-222, (1975). 39 Barna, A., Szigethy, D.: Ion source for generating ions of a gas or vapour. EP0928495, (1996). 40 Kaufman, H.R.: Technology of Electron-Bombardment Ion Thrusters, Adv. Electr. Phys., 36, 265-373, (1974). 41 Voronoi, G.: New applications of continuous parameters in the theory of quadratic forms (in French), J. Reine u. Angew. Math., 134, 198-287, (1908) 42 Delaunay, B.N.: On the Empty Sphere (in French), In: Bull. Acad. Science USSR VII: Class. Sci. Meth., 793-800, (1934). CopyrightGöller Verlag GmbH Acknowledgments |