Technology for the Obtainment of Transparent MgAl2O4 Spinel Parts

A. Goldstein, A. Goldenberg, M. Vulfson

Israel Ceramic and Silicate Institute, Technion City, Haifa 32000, Israel

received May 25, 2010, received in revised form July 12, 2010, accepted September 23, 2010

Vol.2, No.1, Pages 1-8   DOI: 10.4416/JCST2010-00018

Abstract

The objective of the work was the establishment of a procedure allowing the obtainment of high-optical-transparency MgAl2O4 polycrystalline parts that exhibit a fine microstructure (average grains size lower than 5 μm). The technology had to be relevant for industrial-scale production. A nano powder, commercially available in large quantities, at a reasonable price, was used as raw material. It was determined that by applying a suitable combination of powder processing and green-bodies-forming procedure, a configuration favorable for advanced densification can be derived from the selected powder. It was also found that the pore-closing ability of HIPing was best exploited when the specimens subjected to this treatment (predensified by pressureless sintering, in air) exhibited an optimal tradeoff between densification level and microstructural configuration. Specimens combining an average grain size of 2.5 μm with an in-line transmission of 77 % (λ = 750 nm; thickness ∼2 mm) were obtained; such parts possess a Vickers hardness of 13.8 GPa and a transverse rupture strength of ∼200 MPa. Because the technology developed generates transparent spinel exhibiting properties acceptable for some of the existent applications, at reasonable cost, it may be of interest to industry.

Purchase Full Article or get a Subscription

Keywords

Spinel, transparent, ceramic, sintering, armor

References

1 Woosley, J.D., Wood, S., Jander, E., Weeks, R.A.: Photoelectric effects in MgAl2O4 spinel, Phys. Rev., 22, 1065, (1980).

2 Harris, D.C.: History of development of polycrystalline optical spinel in the US, Proc. SPIE, 5786, 1-22, (2005).

3 Goldstein, A., Goldenberg, A., Yeshurun, Y., Hefetz, M.: Transparent MgAl2O4 spinel from a powder prepared by flame spray pyrolysis, J. Am. Ceram. Soc., 91(12), 4141-4144, (2008).

4 Reimanis, I., Kleebe, H.J.: A review on the sintering and microstructure development of transparent spinel (MgAl2O4), J. Am. Ceram. Soc., 92(7), 1472-1480, (2009).

5 Krell, A., Hutzler, T., Klimke, J.: Transparent ceramics for structural applications: part 2, fields of application, cfi Ber. DKG, 84(6), E50-E56, (2007).

6 Cox, J.A., Greenlow, D., Terry, G., Fiedler, L.: Comparative study of advanced IR transmissive materials, Proc. SPIE, 683, 49-61, (1986).

7 Kingery, W.D., Francois, B.: Sintering of Crystalline Oxides I, In: Sintering and Related Phenomena. Kuzcsynski,G.C., Hooton, N.A. and Gibbon G.F. eds, Gordon and Breach, New York, (1967), p. 471.

8 Bratton, R.J.: Translucent sintered MgAl2O4, J. Am. Ceram. Soc., 57(7), 283-286, (1974).

9 Roy, D.W., Hastert, J.L.: Polycrystalline MgAl2O4 spinel for high temperature windows, Ceram. Eng. Sci. Proc., 47(7-8), 502-509, (1983).

10 Hsu, S.E., Wang, C.T., Tsai, D.S., Yang, S.J.: Effect of gas pressure on optical quality of MgAl2O4 spinel, Mat. Res. Soc. Symp. Proc., 251, 257-264, (1992).

11 Roy, D.W., Hastert, J.L., Canbrough, L.E., Green, K.E., Trujillo, A.: Transparent Polycrystalline Body with High UV Transmittance, Process for Making, and Applications Thereof. European Patent 0447390B1, (1994).

12 Bergez, P.: Procedé de Fabrication de Pieces en Spinelle d'Aluminate de Magnesium à Hautes Performances Notamment de Pièces Transparents dans le Domaine de Infrarouge et Visible. European Patent 0334760B1, (1993).

13 Roy, D.W.: Hot pressed MgAl2O4 for UV visible and infrared optical requirements, Proc. SPIE, 297, 13-18, (1981).

14 Gazza, G.E., Dutta, S.K.: Transparent Ultrafine Grained Ceramics. U.S. Patent 4, 029, 755, (1977).

15 Gilde, G., Patel, P., Patterson, P., Blodget, D., Duncan D., Hahn, D.: Evaluation of hot pressing and hot isostatic pressing parameters on the optical properties of spinel, J. Am. Ceram. Soc., 88(10), 2747-2751, (2005).

16 Cheng, J., Agrawal, D., Zhang, Y., Browl, B., Roy, R.: Fabricating transparent ceramics by MW sintering, Am. Ceram. Soc. Bull., 79(9), 71-74, (2000).

17 Dercioglu, A.F., Kagawa, Y.: Effect of grain boundary microcracking on the light transmittance of sintered transparent MgAl2O4, J. Eur. Ceram. Soc., 23, 951-959, (2003).

18 Mroz, T.J., Hartnett, T.M., Wahl, J.M., Goldman, L.M., Kirsch, J., Lindberg, W.R.: Recent advances in spinel optical ceramics, Proc. SPIE, 5786, 64-70, (2005).

19 Goldstein, A., Geifman, L., Bar-Ziv, S.: Susceptor-assisted microwave sintering of MgAl2O4 powder at 2.45 GHz, J. Mat. Sci. Lett., 17(12), 977-979, (1998).

20 Krell, A., Hutzler, T., Klimke, J.: Transparent ceramics for structural applications: part 1, physics of light transmission and technological consequences, cfi Ber. DKG, 84(4), E41-E50, (2007).

21 Goldstein, A., Goldenberg, A., Hefetz, M.: Transparent polycrystalline MgAl2O4 spinel with submicron grains, by low temperature sintering, J. Ceram. Soc. Jpn., 117(11), 1281-1283, (2009).

22 Meir, S., Kalabubkhov, S., Froumin, N., Dariel, M.P., Frage, N.: Synthesis and densification of transparent MgAl2O4 spinel by SPS process, J. Am. Ceram. Soc., 92(2), 358-364, (2009).

23 Lei, M.Y., Huang, C.X., Sin, J.L.: Effect of HIP on the properties and microstructure of transparent polycrystalline spinel, Key Eng. Mat., 336-338, 1200-1202, (2007).

24 Tsukuma, K.: Transparent MgAl2O4 spinel ceramics produced by HIP post-sintering, J. Cer. Soc. Jpn., 114(10), 802-806, (2006).

25 Sweeney, S.M., Brun, M.K., Yosenick, T.J., Kebbede, A., Manohora, M.: High-strength transparent spinel with fine unimodal grain size, Proc. SPIE, 7302, 73020G, (2009).

26 Villalobos, G.R., Sanghera, J.J., Bayya, S.S., Aggarwal, I.: Magnesium aluminate transparent ceramic having low scattering and absorption loss. WO Patent 2006/104540, (2006).

27 West, G.D., Perkins, J.M., Lewis, M.H.: Characterization of fine grained oxide ceramics, J. Mat. Sci., 39, 6687-6704, (2004).

28 Krell, A., Strassburger, E.: Ballistic strength of opaque and transparent armor, Am. Ceram. Soc. Bull., 86(4), 9201-9207, (2007).

29 Hasselman, D.P.H.: Unified theory of thermal shock fracture initiation and crack propagation in brittle ceramics, J. Am. Ceram. Soc., 52(11), 600-604, (1969).

30 Gentilman, R.L.: Fusion casting of transparent spinel, Am. Ceram. Soc. Bull., 60(9), 906-909, (1981).

31 Lu, T.C., Chang, X.H., Qi, J.Q., Lou, X.J., Wei, Q.M., Sun, K., Wang, L.M.: Low temperature high pressure preparation of transparent nanocrystalline MgAl2O4 ceramics, Appl. Phys. Lett., 88, 213120-213123, (2006).

32 Morita, K., Kim, B-N., Hiraga, K., Yashida, H.: Fabrication of transparent MgAl2O4 spinel polycrystal by spark plasma sintering process, Scripta Materialia, 58, 1114-1117, (2008).

33 Udalova, I.V., Maltzev, M.V., Petrik, V.I.: Transparent Spinel Ceramics. In: Proceeding of 3rd Euro Ceramics. Faenza Editrice Iberica, Madrid, (1993), 1, 709-714.

34 Chang, X.H., Lu, T.C., Zhang, Y., Luo, X.J., Liu, Q., Huang, C.B., Qi, J.Q., Lei, M.Y., Huang, C.X., Lin, L.B.: MgAl2O4 transparent nano-ceramics prepared by sintering under ultrahigh pressure, Key Eng. Mat., 280-283, 549-552, (2005).

35 Krell, A., Klimke, J., Hutzler, T.: Advanced spinel and sub-μm Al2O3 for transparent armor applications. J. Eur. Ceram. Soc., 29(2), 275-281, (2009).

36 Lange, F.F.: Sintering of agglomerated powders, J. Am. Ceram. Soc., 67(2), 83-89, (1984).

37 Rahaman, M.N.: Ceramic Processing and Sintering, 2nd edition. Marcel Dekker, New York, (2003).

38 Coble, R.L.: Sintering crystalline solids. I Intermediate and final state diffusion models, J. App . Phys., 32(5), 787-792, (1961).

39 Kang, S-J.L., Jung, Y-L.: Sintering kinetics at final stage sintering: model calculations and map construction, Acta. Mat., 52, 4573-4578, (2004).

40 Yan, M.F., Cannon, R.M., Bowen, H.K., Chowdhry, U.: Effect of grain size distribution on sintered density, Mat. Sci. Eng., 60, 275-281, (1983).

41 Helle, A.S., Easterling, K.E., Ashby, M.F.: Hot isostatic pressing diagrams: new developments, Acta. Metall., 53(12), 2163-2174, (1985).

42 Apetz, R., van Bruggen, M.P.B.: Transparent alumina: a light scattering model, J. Am. Ceram. Soc., 86(3), 480-486, (2003).

43 German, R.M.: Sintering Theory and Practice. J. Wiley & Sons, New York, (1996), p. 316.

44 Kwon, S.T., Kim, D.Y.: Effect of sintering temperature on the densification of Al2O3, J. Am. Ceram. Soc., 70(4), C69-C70, (1987).

Copyright

© 2010 Göller Verlag

 

Printed version

jcst_cover_2013-1

Order journal subscription

© 2009-2013 Göller Verlag GmbH