Effect of Alumina/Iron Catalysts on the Formation of Carbon Nanotubes

Xiaoxue Zhang1, Juha-Pekka Nikkanen1, Jyri Rintala2, Mika Pettersson2, Tomi Kanerva3, Jarmo Laakso3, Erkki Levänen3, Tapio Mäntylä3

1 Department of Materials Science, Tampere University of Technology, P.O. Box 589, FI-33101 Tampere, Finland
2 Nanoscience Center, Department of Chemistry, University of Jyväskylä, P.O Box 35, FI-40014 Jyväskylä, Finland
3 Department of Materials Science, Tampere University of Technology, P.O. Box 589, FI-33101 Tampere, Finland

received April 15, 2010, received in revised form July 07, 2010, accepted July 15, 2010

Vol.1, No.1, Pages 51-54   DOI: 10.4416/JCST2010-00013

Abstract

Two different ferrous compounds, iron nitrate and ferrocene, were applied as the iron precursor in sol-gel processing in order to produce two different iron-containing alumina catalysts. Methane gas was decomposed over the two catalysts under the same conditions to produce carbon nanotubes. Multi-walled carbon nanotubes were formed on the catalyst with iron nitrate, but not obtained on the catalyst produced with ferrocene. X-ray diffraction, transmission electron microscopy, field emission scanning electron microscopy, Raman spectroscopy and nitrogen adsorption/desorption characterization were performed to compare the catalysts and discuss the effect of the catalysts obtained with the different ferrous compounds on the formation of the multi-walled carbon nanotubes.

Purchase Full Article or get a Subscription

Keywords

carbon nanotubes, alumina, sol-gel method, chemical catalytic vapour deposition

References

1 Iijima, S., Helical microtubules of graphitic carbon, Nature, 354, 56-58, (1991)

2 Bethune, D. S., Kiang, C. H., De Vries, M. S., Gorman, G., Savoy, R., Vazquez, J., Beyers, R., Cobalt-catalysed growth of carbon nanotubes with single-atomic-layer walls, Nature, 363, 605-607, (1993)

3 Guo, T., Nikolaev, P., Thess, A., Colbert, D. T., Smalley, R. E., Catalytic growth of single-walled nanotubes by laser vaporization, Chem. Phys. Lett., 243, 49-54, (1995)

4 Tran, K. Y., Heinrichs, B., Colomer, J. F., Pirard, J. P., Lambert, S., Carbon nanotubes synthesis by the ethylene chemical cata­lytic vapour deposition (CCVD) process on Fe, Co, and Fe-Co/Al2O3 sol-gel catalysts, Appl. Catal. A, 318, 63-69, (2007)

5 Ren, Z. F., Huang, Z. P., Xu, J. W., Wang, J. H., Bush, P., Siegas, M. P., Provencio, N., Synthesis of large arrays of well-aligned carbon nanotubes on glass, Science, 282, 1105-1107, (1998)

6 Gan, S., Chapline, M. G., Franklin, N. R., Tombler, T. W., Cassen, A. M., Dai, H., Self-oriented regular arrays of carbon nanotubes and their field emission properties, Science, 283, 512-514, (1999)

7 Fazle Kibria, A.K.M., Mo, Y.H., Nahm, K.S., Kim, M.J., Synthesis of narrow- diameter carbon nanotubes from acetylene decomposition over an iron-nickel catalysts supported on alumina, Carbon, 40, 1241-1247, (2002)

8 Kathyayini H., Willems I., Fonseca A., Nagy J. B. and Nagaraju N., Catalytic materials based on alumina hydroxide, for a large scale production of bundles of multiwalled (MWNT) carbon nanotubes, Catal. Commun., 7, 140-147, (2006)

9 Ciambelli, P., Sannino, D., Sarno, M., Leone, C., Lafont, U., Effects of alumina phases and process parameters on the multi­walled carbon nanotubes growth, Diamond Relat. Mater., 16, 1144-1149, (2007)

10 Nagaraju N., Fonseca A., Konya Z. and Nagy J. B., Alumina and Silica Supported Metal Catalysts for the Production of Carbon Nanotubes, J. Mol. Catal. A: Chem., 181, 57-62, (2002)

11 Corriu R., Mehdi A. and Reye C., Nanoporous materials: a good opportunity for nanosciences, J. Organomet. Chem., 689, 4437-4450, (2004)

12 Farag H. K. and Endres F., Studies on the synthesis of nano-alumina in air and water stable ionic liquids, J. Mater. Chem., 18, 442-449, (2008)

13 Lecloux A. J. and. Pirard J. P, High-temperature catalysts through sol-gel synthesis, J. Non-Cryst. Solids, 225, 146-152, (1998)

14 Zhang, X., Honkanen, M., Levänen, E., Mäntylä, T., Transition Alumina Nanoparticles and Nanorods from boehmite nanoflakes, J. Cryst. Growth, 310, 3674-3679, (2008)

15 Zhang, X., Ge, Y., Hannula, S., Levänen, E., Mäntylä, T., Nanocrystalline a- alumina with novel morphology at 1000 °C, J. Mater. Chem., 18, 2423-2425, (2008)

16 Zhang, X., Ge, Y., Hannula, S., Levänen, E., Mäntylä, T., Process study on the formation of nanocrystalline a-alumina with novel morphology at 1000 °C, J. Mater. Chem., 19, 1915-1922, (2009)

17 Jorio, A., Pimenta, M. A., Souza Filho, A. G., Saito, R., Dresselhaus, G., Dresselhaus, M. S., Characterizing carbon nanotube samples with resonance Raman scattering, New J. Phys., 5, 139.1-139.17, (2003)

18 Araujo, P. T., Doorn, S. K., Kilina, S., Tretiak, S., Einarsson, E., Maruyama, S., Chacham, H., Pimenta, A. M., Jorio, A., Third and fourth optical transitions in semiconducting carbon nanotubes, Phys. Rev. Lett., 98, 67401, 8 pages, (2007)

19 DiLeo, R. A., Landi, B. J., Raffaelle, R. P., Purity assessment of multiwalled carbon nanotubes by Raman spectroscopy, J. Appl. Phys., 101, 64307-64311, (2007)

Copyright

© 2010 Göller Verlag

Acknowledgments

The present study was supported by an EU research project IP NANOKER (FP6-515784-2), the Academy of Finland (decision no. 117937) and the Finnish National Graduate School on New Materials and Processes.

 

Printed version

jcst_cover_2013-1

Order journal subscription

© 2009-2013 Göller Verlag GmbH